DYMAX 6-621-VT

Main features

  • High-Viscosity Bead Retention
  • Multi-Cure Joint Accessibility
  • Structural Battery Bonding Fit

Product Description

Dymax Multi-Cure 6-621-VT Adhesive is the high-viscosity member of the 6-621 structural adhesive family. The thicker flow profile supports applications that need improved bead retention or reduced movement after dispensing, while UV and visible light provide the primary cure route on exposed material. Secondary heat and compatible activator cure extend processing into shadowed bond areas. The adhesive is used for bonding phenolic and filled plastics, glass, and metals, with applications including metal-to-glass assembly, coil winding, potting, and structural battery bonding. Its main selection distinction is higher pre-cure viscosity within a shared multi-cure platform.

Key features

  • High-viscosity bead retention: The VT grade is selected where a thicker, more stationary adhesive profile is useful.
  • Multi-Cure process coverage: UV/visible, heat, and activator routes address exposed and shadowed regions.
  • Structural family compatibility: The documented scope includes phenolic materials, glass, metals, and battery assemblies.

Applications / Suitable for

  • Metal-to-glass bonding
  • Coil winding and potting
  • Structural battery bonding
Product Family

DYMAX 6-621-VT

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear Translucent Liquid - Gel
Refractive index
1.51
Thermal Properties
Glass Transition Temperature (Tg)
75 °C
Chemical Properties
Water Absorption
1.7 %

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics for the high-viscosity 6-621 family variant.

Property Value Unit Method / condition
Viscosity class High As supplied
Placement behavior Thick, bead-retaining profile Before cure
Primary cure activation UV and visible light Exposed adhesive areas
Secondary cure option Heat Areas with limited light access
Activator cure option Compatible activator Close-fitting or shadowed joints
Technical properties

After-processing / final-state properties

Cured-state function and Bonded-material scope.

Property Value Unit Method / condition
Final function Structural bonded joint After complete cure
Bonded material scope Phenolic and filled plastics; glass; metal Substrate range
Bondline character Retained localized bondline After curing the high-viscosity placement
Assembly roles Coil winding; potting Within the Application scope
Battery assembly role Structural battery bonding Within the Application scope