DYMAX 3089-GEL

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 3089-GEL

Main features

  • Low-Stress Flexible Laminating
  • Gel-Form Placement Control
  • Glass, Metal, and Plastic Bonding

Product Description

Dymax 3089-GEL Low-Stress Bonding / Laminating Adhesive combines a gel consistency with fast UV- and visible-light cure for low-stress bonding and laminating. The flexible cured adhesive joins glass, plastics, metals, nickel, and Mylar polyester within the supported substrate range. Its gel form is suited to applications where controlled placement is preferred, while the cured flexibility accommodates assemblies that should not be constrained by a rigid bondline. The material can also be used in sealing and gasketing tasks identified for the product. Applications include flexible laminations, glass or metal assemblies, and bonding to Mylar polyester and nickel surfaces.

Key features

  • Low-stress cured flexibility: The flexible cured material is suited to laminating and movement-tolerant assemblies.
  • Controlled gel placement: The gel consistency supports localized application before light cure.
  • Multi-material adhesion: Bonds glass, plastics, metals, nickel, and Mylar polyester within the supported scope.

Applications / Suitable for

  • Low-stress bonding and laminating
  • Glass, plastic, and metal assembly
  • Sealant and gasketing applications
Product Family

DYMAX 3089-GEL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear/Straw Liquid
Refractive index
1.492
Thermal Properties
Flash Point
>93 °C
Chemical Properties
Water Absorption
3.6 %

Additional Information

Technical properties

As-supplied / before-processing properties

Exact-product as-supplied characteristics relevant to placement and light-cure processing.

Property Value Unit Method / condition
Physical form Gel As supplied
Cure activation UV and visible light Exposed adhesive
Cure response Fast Light-cure processing
Placement behavior Localized and controlled Gel-form application
Technical properties

After-processing / final-state properties

Exact-product final-state characteristics and supported joint scope.

Property Value Unit Method / condition
Cured material character Flexible After light cure
Bonding mode Low-stress bonding and laminating Cured joint
Bonded substrate scope Glass; plastics; metals; nickel; Mylar polyester Within the listed substrate scope
Secondary joint role Sealing and gasketing Where specified for the product