DYMAX 3069

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 3069

Main features

  • Flexible Plastic Lamination
  • UV/Visible-Light Assembly Cure
  • Multi-Substrate Plastic Bonding

Product Description

Dymax 3069 Flexible Laminating and Plastic Bonding Adhesive is a UV- and visible-light-curable acrylated urethane adhesive for flexible lamination and plastic assembly. It bonds supported substrates including PVC, polycarbonate, polyurethane, PET, PETG, and ABS, allowing one material to address several common plastic combinations within a validated light-cure process. The adhesive supports flexible laminates, plastic housings, appliance assemblies, and speaker components. Its light-activated cure supports controlled production where the bond area can receive the required UV or visible-light exposure. This application range makes the product relevant for plastic assemblies that combine flexible layers with rigid molded parts.

Key features

  • UV/visible-light cure: Light activation supports controlled curing in accessible plastic joints.
  • Flexible lamination: Formulated for laminating flexible plastic layers and assemblies.
  • Documented plastic range: Bonds PVC, polycarbonate, polyurethane, PET, PETG, and ABS.

Applications / Suitable for

  • Flexible plastic lamination
  • Plastic housing and appliance assembly
  • Speaker component assembly
Product Family

DYMAX 3069

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear Translucent Liquid
Refractive index
1.51
Thermal Properties
Glass Transition Temperature (Tg)
68 °C
Chemical Properties
Water Absorption
1.6 %

Additional Information