DOWSIL TC-6032

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL TC-6032

Main features

  • Extended-Flow Electronic Encapsulation
  • 3.2 W/(m K) Thermal Protection
  • EV Power-Component Encapsulation

Product Description

DOWSIL TC-6032 Thermally Conductive Encapsulant is a two-part blue silicone encapsulant for thermal management and protection in electric-vehicle power electronics. The 1:1 system has a typical mixed viscosity of 6,500 mPa s and a 240-minute pot life at 25 deg C, providing extended flow and impregnation time before heat cure. Typical cure schedules include 60 minutes at 80 deg C, 30 minutes at 100 deg C, or 20 minutes at 120 deg C. The cured material combines 3.2 W/(m K) bulk thermal conductivity with Shore A 34 hardness, 45% elongation, and aluminum-to-aluminum lap shear strength of 0.38 MPa. It is used in on-board chargers, DC/DC converters, inductors, and transformers.

Key features

  • Extended flow window: A 240-minute pot life at 25 deg C supports impregnation and complex dispensing.
  • High thermal conductivity: The cured bulk material provides 3.2 W/(m K) thermal conductivity.
  • Compliant cured material: Shore A 34 hardness and 45% elongation characterize the cured encapsulant.

Applications / Suitable for

  • On-board chargers
  • DC/DC converters
  • Inductors and transformers

Technical Specifications

General Properties
Color
White / blue
Component System
Two (A / B)
Mix Ratio
1 to 1
Pot Life
4 hours
Specific Gravity
2.72
Mechanical Properties
Elongation
45 %
Thermal Properties
Thermal Conductivity
3.2 W/m.K
Electrical Properties
Dielectric Strength
18 kV/mm
Volume Resistivity
1.3 x 10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical mixed-system properties and heat-cure windows before cure.

Property Value Unit Method / condition
Number of parts 2 Part A and Part B
Mix ratio 1:1 By weight
Component colors White; blue Part A; Part B
Mixed color Blue After mixing
Mixed viscosity 6,500 mPa s Typical
Pot life 240 min At 25 deg C
Heat-cure schedule 60 min At 80 deg C
Heat-cure schedule 20 min At 120 deg C
Technical properties

After-processing / final-state properties

Typical properties of the cured encapsulant; thermal conductivity is a bulk-material value.

Property Value Unit Method / condition
Density 2.73 g/cm^3 Cured material
Durometer hardness 34 Shore A Cured material
Thermal conductivity 3.2 W/(m K) Cured bulk material
Tensile strength 0.5 MPa Cured material
Elongation 45 % Cured material
Lap shear strength 0.38 MPa Aluminum-to-aluminum