DOWSIL TC-5121C

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DOWSIL TC-5121C

Main features

  • 2.8 W/(m K) Thermal Interface
  • 0.09 deg C cm^2/W Thermal Resistance
  • One-Part, Non-Curing and Flowable Formulation

Product Description

DOWSIL™ TC-5121 C Thermally Conductive Compound is a one-part, flowable, non-curing silicone thermal compound designed to transfer heat between electrical devices or PCB system assemblies and a heat sink or chassis. Its filled polydimethylsiloxane formulation provides typical thermal conductivity of 2.8 W/m·K and thermal resistance of 0.09°C·cm²/W at 40 psi. The compound can form thin bondlines and may be applied by dispensing, screen printing, or stencil printing. :contentReference[oaicite:0]{index=0}

Key features

  • Effective thermal transfer: Provides typical thermal conductivity of 2.8 W/m·K and low thermal resistance at a defined pressure.
  • Non-curing formulation: Requires no curing oven and remains a grease-like thermal-interface compound after installation.
  • Thin-bondline capability: Flowable consistency supports screen printing, stencil printing, and dispensing for controlled interface application.

Applications / Suitable for

  • Thermal interfaces in mid- to high-end PCB system assemblies
  • Heat transfer from electrical devices to heat sinks or chassis
Product Family

DOWSIL TC-5121C

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Greenish Yellow
Component System
One
Specific Gravity
4.2
Physical Properties
Thixotropic index
1.69
Viscosity
79000 mPa.s
Thermal Properties
Thermal Conductivity
2.8 W/m.K
Electrical Properties
Dielectric Strength
1.89 kV/mm
Volume Resistivity
1.3E+13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties of DOWSIL TC-5121 C Thermally Conductive Compound. Values are not intended for specification purposes. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Number of components 1 part As supplied
Composition Filled polydimethylsiloxane — Product composition
Color Greenish yellow — As supplied
Viscosity 79.0 (79,000) Pa·s (cP) CTM 0050; temperature and shear conditions not stated
Thixotropy 1.69 — CTM 0905
Specific gravity 4.2 — Uncured; CTM 0540
Non-volatile content 99.93 % Test method and conditions not stated
Technical properties

After-processing / final-state properties

Typical thermal and electrical properties of the non-curing compound. Values are not intended for specification purposes. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
Thermal conductivity 2.8 W/m·K CTM 1388; temperature and specimen conditions not stated
Thermal resistance 0.09 °C·cm²/W At 40 psi; method and bondline thickness not stated
Dielectric strength 1.89 (47.3) kV/mm (V/mil) CTM 0114; specimen thickness and conditioning not stated
Volume resistivity 1.3 × 1013 ohm·cm CTM 1400
Dielectric constant 14.0 — At 1 kHz; CTM 1139
Dissipation factor 0.073 — At 1 kHz; CTM 1139