DOWSIL SE4400

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL SE4400

Main features

  • Extended 17-Hour Working Window
  • Accelerated 30-Minute Heat Cure
  • Thermally Conductive PCB Bonding

Product Description

DOWSIL SE 4400 Thermally Conductive Adhesive is a two-part gray silicone adhesive for thermal bonding in PCB system assembly modules. The flowable 1:1 mix has a typical mixed viscosity of 62,500 mPa s and a 17-hour working time at 25 deg C, providing an extended window for mixing, dispensing, and assembly. Heat cure is accelerated to 30 minutes at 150 deg C, and the addition-cure system produces no cure by-products, allowing deep-section and confined curing. The cured material has 0.92 W/(m K) thermal conductivity and 2.72 MPa unprimed lap shear strength on aluminum for combined heat transfer and attachment.

Key features

  • Extended working window: A typical 17-hour working time at 25 deg C supports longer dispensing and assembly operations.
  • Accelerated heat cure: Typical cure time is 30 minutes at 150 deg C.
  • Thermal and bond performance: Cured bulk thermal conductivity is 0.92 W/(m K), with 2.72 MPa unprimed lap shear on aluminum.

Applications / Suitable for

  • Thermal bonding in PCB system assembly modules
  • Cooling assemblies that require combined attachment and heat transfer
Product Family

DOWSIL SE4400

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
Color
Gray
Component System
Two
Specific Gravity
2.15
Mechanical Properties
Elongation
85 %
Electrical Properties
Dielectric Strength
25 kV/mm
Volume Resistivity
5.0E+15 Ohms⋅cm
Thermal Properties
Thermal Conductivity
0.92 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the mixed adhesive before cure.

Property Value Unit Method / condition
Number of parts Two Product configuration
Mix ratio 1:1 Part A to Part B
Color Gray As mixed
Mixed viscosity 62,500 mPa s Typical
Working time 17 hours At 25 deg C
Heat cure time 30 min At 150 deg C
Technical properties

After-processing / final-state properties

Typical properties of the heat-cured adhesive.

Property Value Unit Method / condition
Durometer hardness 79 Shore A Cured
Specific gravity 2.15 Cured
Tensile strength 5.6 MPa Cured
Elongation 85 % Cured
Unprimed lap shear 2.72 MPa Aluminum
Dielectric strength 25 kV/mm Cured
Thermal conductivity 0.92 W/(m K) Cured bulk material