DOWSIL SE 9186 Sealant

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL SE 9186 Sealant

Main features

  • Fast Room-Temperature Sealing Cure
  • Self-Leveling Flowable Placement
  • Controlled-Volatility Silicone Formulation

Product Description

DOWSIL™ SE 9186 Black, Clear or White Adhesive is a one-part, moisture-curing silicone adhesive-sealant that cures at room temperature to a soft, low-stress elastomer. Formulated with controlled silicone volatility and a flowable, self-leveling consistency, this solventless adhesive is engineered specifically for sealing electronic equipment and fixing parts on circuit boards. Its fast tack-free time helps accelerate in-line processing without the need for curing ovens, enhancing overall manufacturing throughput.

Key features

  • Fast room temperature cure: Tack-free in 8 minutes, enabling faster in-line processing without ovens while allowing for heat acceleration if desired.
  • Flowable and self-leveling: Easily fills gaps and levels itself after dispensing, making it ideal for complex circuit board geometries.
  • Controlled volatility: Reduced potential for silicone volatiles protects sensitive electronic modules and components.

Applications / Suitable for

  • Sealing of electronic equipment and modules
  • Parts fixing on circuit boards
  • Sealing against potential stress cracks

Technical Specifications

General Properties
Color
Black, Translucent or White
Component System
1k
Specific Gravity
1.35
Physical Properties
Viscosity
64,000 mPa.s
Mechanical Properties
Elongation
550 %
Physical Properties
Tack-Free Time
8 minutes
Electrical Properties
Dielectric Strength
23 kV/mm
Volume Resistivity
2.0 E+16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color Black, Translucent or White - One-part
Viscosity 64,000 cP -
Tack-Free Time 8 minutes at 25°C
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Specific Gravity 1.03 - Cured
Durometer 20 Shore A -
Tensile Strength 360 psi -
Elongation 550 % -
Adhesion Lap Shear 185 psi Glass
Dielectric Strength 575 volts/mil -
Volume Resistivity 2.0E+16 ohm*cm -