DOWSIL RSN-0806

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL RSN-0806

Main features

  • Colored Baking-Enamel Resin
  • Up to 538 deg C Temperature Use
  • Standalone or Blendable Resin Use

Product Description

DOWSIL™ RSN-0806 Resin is a silanol-functional silicone binder resin supplied as a 50% solids, solvent-borne solution for high-temperature coating formulations. It is designed primarily for colored baking enamels used on space heaters, stoves, and similar equipment. The resin provides stability and high-temperature performance and may be used alone or blended with DOWSIL™ RSN-0805 Resin to enhance coating flexibility.

Key features

  • High-temperature coating binder: Supports coating formulations intended for service at temperatures up to 538°C (1000°F).
  • Silanol-functional resin: Provides a reactive silicone binder for heat-cured coating systems.
  • Formulation versatility: Can be used alone or blended with DOWSIL™ RSN-0805 Resin to enhance film flexibility.
  • Pre-catalyzed formulation: Supplied with catalyst to support heat-curing applications.

Applications / Suitable for

  • Colored baking enamels
  • High-temperature coatings for space heaters
  • High-temperature coatings for stoves and similar equipment
Product Family

DOWSIL RSN-0806

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.02
Physical Properties
Viscosity
150 mPa.s
Thermal Properties
Flash Point
45 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Composition Silanol-functional silicone resin in solvent — As supplied; pre-catalyzed
Diluent Toluene/xylene — As supplied
Resin solids 50 % by weight 0.5 g, 1 hour at 110°C (230°F)
Resin solids by volume 41 % Typical value
Dynamic viscosity 150 cP Typical value
Specific gravity 1.02 — At 25°C (77°F)
Volatile organic content 515 (4.3) g/L (lb/gal) EPA Reference Method 24
Flash point, closed cup 7 (45) °C (°F) Closed cup
Theoretical silicon dioxide content 52 % By weight
Phenyl/methyl ratio 1.2/1.0 — Typical value
Degree of substitution 1.4 — Organic groups attached per silicon atom
Shelf life 1080 days From date of manufacture when stored in the original unopened container