DOWSIL Q4-2817 FLUOROSILICONE SEALANT

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL Q4-2817 FLUOROSILICONE SEALANT

Main features

  • 55 to 260 deg C Service Range
  • Aviation-Fuel, Fuel, and Solvent Resistance
  • Aerospace Sealing Application

Product Description

DOWSIL™ Q4-2817 Fluorosilicone Sealant is a one-part, ready-to-use, high-strength solventless fluorosilicone elastomer paste that cures at room temperature to form a tough, rubbery solid. Developed for equipment exposed to solvents, oil, and fuels, this sealant protects surfaces from erosion and corrosion while maintaining flexibility across a broad temperature range of -55°C to +260°C. It is highly suitable for evaluation in aerospace applications, including the critical sealing of aircraft fuel tanks.

Key features

  • Fluid resistance: Retains its physical properties when exposed to aviation fuels, oils, and solvents.
  • Environmental stability: Offers excellent resistance to weathering, moisture, ozone, and extreme temperatures from -55°C to +260°C.
  • Easy application: Features a one-part, room-temperature curing system that adheres well to most materials.

Applications / Suitable for

  • Sealing aircraft fuel tanks
  • Bonding or sealing components exposed to moisture, vibration, shock, fuel, and solvents
  • Protecting surfaces exposed to fuel from erosion and corrosion
Product Family

DOWSIL Q4-2817

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Red
Density
1.8 kg/m3
Solids
97 %
Physical Properties
Skin Time
11 minutes
Mechanical Properties
Elongation
375 %
Physical Properties
Extrusion Rate
120 g/min
Tack-Free Time
40 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color Red - As supplied, at 25°C and 50% relative humidity
Relative Density 1.8 - at 25°C (CTM 0022 / ASTM D792)
Skin-over Time 11 minutes As supplied, at 25°C and 50% relative humidity (CTM 0098)
Extrusion Rate 120 g/minute 3 mm orifice, 0.6 MPa air (CTM 0364)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications[cite: 3].

Property Value Unit Method / condition
Durometer Hardness 43 Shore A As cured after 14 days at 25°C and 50% RH (CTM 0099 / ASTM D2240)
Tensile Strength 4.5 MPa As cured after 14 days at 25°C and 50% RH (CTM 0137A / ASTM D412)
Elongation at Break 375 % As cured after 14 days at 25°C and 50% RH (CTM 0137A / ASTM D412)[
Tear Strength 15 kN/m Die B, as cured after 14 days at 25°C and 50% RH (CTM 0159A / ASTM D624)
Peel Strength 10.5 kN/m As cured after 14 days at 25°C and 50% RH (CTM 0293)