DOWSIL Q3-6611

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL Q3-6611

Main features

  • Self-Leveling Flowable Dispensing
  • Temperature-Controlled Rapid Cure
  • High Tensile Strength

Product Description

DOWSIL™ Q3-6611 Adhesive is a one-part, heat-curing silicone adhesive formulated for electronic and automotive assembly applications requiring flowability, adhesion, and mechanical durability. The material is designed to flow, fill, and self-level after dispensing, enabling efficient sealing, gasketing, and component attachment processes. With no mixing required and cure speed controlled by temperature, DOWSIL™ Q3-6611 supports flexible manufacturing operations. The cured adhesive provides high tensile strength, unprimed adhesion to aluminum, and reliable performance across a broad operating temperature range, making it suitable for demanding assemblies including engine controllers, ABS modules, transmission controllers, connectors, and lighting systems.

Key features

  • One-part heat-cure silicone: Eliminates mixing requirements while allowing cure speed to be adjusted through processing temperature.
  • Flowable, self-leveling behavior: Flows and fills after dispensing to support sealing, gasketing, and component attachment applications.
  • High-strength adhesion: Delivers approximately 850 psi lap shear adhesion to aluminum after cure.

Applications / Suitable for

  • Sealing lids and housings
  • Attaching baseplates
  • Gasketing applications
  • Connector sealing
  • Engine controller assemblies
  • ABS and transmission controller assemblies
  • Automotive and industrial lighting assemblies

Technical Specifications

General Properties
Color
Black / Gray
Specific Gravity
1.32 / 1.31
Physical Properties
Viscosity
92375 / 87025 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for the black grade prior to cure. Values are typical data and not specifications.

Property Q3-6611 (Black) Q3-6611 (Gray) Unit Method / condition
Viscosity 92.4 87 Pa·s Typical value
Heat cure time 180 - minutes 100°C
Heat cure time 60 60 minutes 125°C
Heat cure time 30 30 minutes 150°C
Shelf life 12 12 months Stored at 5°C
Technical properties

After-processing / final-state properties

Typical cured properties for the black grade. Values are typical data and not specifications.

Property Q3-6611 (Black) Q3-6611 (Gray) Unit Method / condition
Specific gravity 1.32 1.31 - Cured
Durometer hardness 60 59 Shore A Typical value
Lap shear adhesion to aluminum 850 880 psi Unprimed adhesion
Hardening transition by DSC -46 - °C DSC measurement
Linear CTE - 250 ppm/°C  TMA
Recommended operating range -45 to 200 -45 to 200 °C Long-term operation