DOWSIL Q3-3384-1

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL Q3-3384-1

Main features

  • Visual 10:1 Mix Verification
  • Fast Room-Temperature Handling
  • Non-Self-Leveling Component Sealing

Product Description

DOWSIL Q3-3384-1 Base with SILASTIC Q3-3636 Special Black Catalyst is a two-component, room-temperature-curing thixotropic silicone adhesive system for durable component sealing. The off-white base and black catalyst provide visual confirmation of mixing at the required 10:1 ratio by weight. Its non-self-leveling paste consistency supports controlled placement, while typical snap time is 8 to 11 minutes and tack-free time is 15 to 20 minutes. After seven days at room temperature, the cured adhesive has Shore A 33 hardness, 1.6 MPa tensile strength, and 250% elongation. The system uses a neutral alkoxy cure and is intended for adhesive sealing of components.

Key features

  • Visual mix verification: Contrasting off-white base and black catalyst make incomplete mixing easier to identify.
  • Fast room-temperature handling: Typical 8 to 11 minute snap time and 15 to 20 minute tack-free time support rapid handling.
  • Thixotropic sealing paste: Non-self-leveling consistency supports controlled adhesive sealing of components.

Applications / Suitable for

  • Durable adhesive sealing of components
Product Family

DOWSIL Q3-3384-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Off white/yellow | Black
Component System
DOWSIL™ Q3-3384-1 Base | SILASTIC™ Q3-3636 Special Black Catalyst
Specific Gravity
1.2 | 1.04
Physical Properties
Tack-Free Time
15–20 minutes
Mechanical Properties
Elongation
250 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system properties before cure.

Property Value Unit Method / condition
Component appearance Off-white/yellow base; black catalyst CTM 0176
Base viscosity 84,500 mPa s CTM 0050
Base specific gravity 1.2 CTM 0097
Catalyst consistency 180 to 460 mm/10 Penetration test
Catalyst specific gravity 1.04 CTM 0097
Mix ratio 10:1 Base to catalyst by weight
Snap time 8 to 11 min As mixed
Tack-free time 15 to 20 min As mixed; CTM 0095
Technical properties

After-processing / final-state properties

Typical cured properties after 7 days at room temperature.

Property Value Unit Method / condition
Durometer hardness 33 Shore A CTM 0099
Tensile strength 1.6 MPa CTM 0137A
Elongation 250 % CTM 0137A

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers