DOWSIL Q2-7406

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL Q2-7406

Main features

  • Silicone PSA Tape Coating
  • High-Temperature Tape Adhesion
  • Adjustable Tack-Cohesion Balance

Product Description

DOWSIL Q2-7406 Adhesive is a solvent-borne silicone pressure-sensitive adhesive for coating tape backings. The translucent xylene dispersion contains 55 to 58% active ingredients and has a typical viscosity of 20,000 to 80,000 cP at 25 deg C. It can be applied with conventional tape-coating equipment, diluted with compatible solvents, or blended with other silicone pressure-sensitive adhesives before coating. After solvent removal, heat cure develops the film's tack, adhesive strength, and cohesive strength. Applications include general-purpose adhesive use and the production of splicing and plating tapes for elevated-temperature service.

Key features

  • Tape-coating processability: Can be applied to backing materials with conventional tape-coating equipment.
  • High-temperature adhesion: Supports splicing and plating tape applications exposed to elevated processing temperatures.
  • Adjustable cure balance: Catalyst concentration and heat cure can be used to balance tack, adhesive strength, and cohesive strength.

Applications / Suitable for

  • General-purpose pressure-sensitive adhesive coating
  • Splicing tapes
  • Plating tapes
Product Family

DOWSIL Q2-7406

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent
Specific Gravity
0.98
Physical Properties
Viscosity
20,000 - 80,000 mPa.s
Thermal Properties
Flash Point
27 °C
Electrical Properties
Volume Resistivity
3.5 x 10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the adhesive dispersion as supplied.

Property Value Unit Method / condition
Appearance Translucent As supplied
Diluent Xylene As supplied
Active ingredients 55 to 58 % Typical
Viscosity 20,000 to 80,000 cP At 25 deg C
Specific gravity 0.98 At 25 deg C
Flash point 27 deg C Closed cup
Usable life 24 months At or below 32 deg C in original unopened containers
Technical properties

After-processing / final-state properties

Typical electrical properties of the cured adhesive film after 96 hours at 23 deg C and 50% relative humidity.

Property Value Unit Method / condition
Electric strength 653 V/mil 2 mil film on aluminum panel; 6.35 mm electrodes
Dielectric constant 2.93 At 10^2 Hz
Dielectric constant 2.87 At 10^5 Hz
Dissipation factor 0.004 At 10^2 Hz
Dissipation factor 0.001 At 10^5 Hz
Volume resistivity 3.5 x 10^14 ohm cm Cured adhesive film