DOWSIL Q1-4010 CONFORMAL COATING

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL Q1-4010 CONFORMAL COATING

Main features

  • One-Part, Solventless Silicone Coating
  • Multiple Supported Application Methods
  • UV-Aided Coating Inspection

Product Description

DOWSIL™ Q1-4010 Conformal Coating is a one-part, transparent silicone conformal coating for protecting rigid and flexible circuit boards, printed wiring boards, and assemblies containing sensitive components or fine-pitch designs. The medium-viscosity, solventless material can be applied by dip, spray, brush, flow, or automated pattern coating and uses temperature-controlled heat curing for rapid processing. After cure, it forms a soft, low-stress elastomer with electrical insulation properties. A built-in UV indicator supports visual or automated inspection of coating coverage. The product is listed to IPC-CC-830B and UL 746E, classified UL 94 V-1, and tested to MIL-I-46058C Amendment 7.

Key features

  • Rapid heat cure: Typical cure time is 10 minutes after the coating reaches 100°C, with actual time dependent on film thickness, oven type, and board thermal mass.
  • Soft silicone protection: Cures to a 33 Shore A, low-stress elastomer with a typical dielectric strength of 23 kV/mm.
  • Inspection and qualification support: Contains a UV indicator and carries IPC-CC-830B, UL 746E, UL 94 V-1, and MIL-I-46058C Amendment 7 credentials.

Applications / Suitable for

  • Rigid and flexible circuit boards
  • Printed wiring boards
  • Boards with sensitive components and fine-pitch designs
Product Family

DOWSIL Q1-4010

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
825 mPa.s
General Properties
Specific Gravity
1
Electrical Properties
Dielectric Strength
23 kV/mm
Volume Resistivity
2.11 E14 Ohms⋅cm
Thermal Properties
UL 94 Rating
V-1

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties; values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Product form One-part liquid — As supplied
Color Transparent — As supplied
Viscosity 825 mPa·s Typical value; equivalent to 825 cP
Non-volatile content 99 % Typical property
Shelf life 12 months Stored at 5°C; observe the product-label use-before date
Technical properties

After-processing / final-state properties

Typical cured-material properties; values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Heat-cure time 10 minutes After the coating reaches 100°C; film thickness, oven type, and board thermal mass affect actual time
Specific gravity 1.00 — Cured material
Hardness 33 Shore A Cured material
Unprimed lap-shear adhesion 130 / 0.9 / 9 psi / MPa / kg/cm² Aluminum substrate; unprimed lap-shear test
Dielectric strength 575 / 23 V/mil / kV/mm Typical cured-material property; not a working-voltage rating
Volume resistivity 2.11 × 1014 Ω·cm Typical cured-material property
Dielectric constant 2.85 / 2.63 — At 100 Hz / 100 kHz, respectively
Dissipation factor 0.00271 / 0.0003 — At 100 Hz / 100 kHz, respectively