DOWSIL PV-801

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL PV-801

Main features

  • Non-Slump PV Frame Sealing
  • 746% Elongation for Flexible Sealing
  • Glass and Backsheet Junction-Box Bonding

Product Description

DOWSIL PV-801 Neutral Sealant is a one-part, neutral alkoxy-cure silicone adhesive and sealant for photovoltaic module assembly. The non-slump paste can be extruded at a typical rate of 197 g/min through a 3.18 mm nozzle at 0.62 MPa and skins over in about 10 to 15 minutes at room temperature and 50% relative humidity. After seven days under those conditions, the cured sealant has 746% elongation at break, 1.69 MPa tensile strength, and Shore A 28 hardness. Applications include photovoltaic frame sealing and junction-box bonding to glass and plastic backsheets.

Key features

  • Non-slump application: Paste consistency supports controlled bead placement for module sealing and bonding.
  • High cured elongation: Typical 746% elongation at break provides an elastic cured seal for photovoltaic assemblies.
  • PV assembly fit: Used for module frame sealing and junction-box bonding to glass and plastic backsheets.

Applications / Suitable for

  • Photovoltaic module frame sealing
  • Junction-box bonding to glass
  • Junction-box bonding to plastic backsheets
Product Family

DOWSIL PV-801

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White or bright white
Specific Gravity
1.51
Physical Properties
Extrusion Rate
210 g/min
Tack-Free Time
55 minutes
Mechanical Properties
Elongation
556 %
Electrical Properties
Dielectric Strength
> 19 kV/mm
Volume Resistivity
4×10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical handling and application properties before cure.

Property Value Unit Method / condition
Color White or bright white CTM 0176
Consistency Non-slump paste As supplied
Extrusion rate 197 g/min 3.18 mm nozzle at 0.62 MPa; CTM 0364 / ASTM D2452
Skin-over time About 10 to 15 min Room temperature and 50% relative humidity
Technical properties

After-processing / final-state properties

Typical cured properties after 7 days at 23 deg C and 50% relative humidity.

Property Value Unit Method / condition
Specific gravity 1.51 At 23 deg C; CTM 0022 / ASTM D792
Durometer hardness 28 Shore A CTM 0099 / ASTM D2240
Tensile strength 1.69 MPa CTM 0137A / ASTM D412
Elongation at break 746 % CTM 0137A / ASTM D412
Modulus at 100% 0.43 MPa CTM 0137A / ASTM D412
Tear strength, Die B 9.8 kN/m CTM 0159A / ASTM D624
Dielectric strength 13 kV/mm CTM 0114 / ASTM D149
Volume resistivity 2.1 x 10^14 ohm cm CTM 0249 / ASTM D257