DOWSIL OS-30

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL OS-30

Main features

  • Complete Low-Residue Room-Temperature Evaporation
  • Low-Surface-Tension Precision Cleaning
  • Most-Plastic and Coating Compatibility

Product Description

DOWSIL™ OS-30 Fluid is a clear, colorless, and odorless methyl polysiloxane fluid used for precision cleaning, rinsing, and process-carrier applications. Its low surface tension supports wetting of complex surfaces, while its mild cleaning action is compatible with most plastics and delicate surface coatings. The fluid evaporates completely at room temperature and has very low residual nonvolatile content, allowing cleaned surfaces to be subsequently painted, coated, or bonded. Applications include removing nonvolatile silicone contamination, rinsing parts after stronger cleaning processes, impregnating cleaning wipes, cleaning industrial optics and spectacle lenses, and carrying silicone oils or greases.

Key features

  • Complete evaporation: Evaporates at room temperature with very low residual nonvolatile content, supporting subsequent coating, painting, or bonding operations.
  • Low surface tension: A typical surface tension of 17.3 dynes/cm at 25°C supports wetting during cleaning and carrier applications.
  • Broad material compatibility: Compatible with most plastics and surface coatings, including delicate coatings, subject to application-specific compatibility testing.

Applications / Suitable for

  • Rinsing parts after cleaning with stronger cleaning agents
  • Removing nonvolatile silicone contamination before painting, coating, or bonding
  • Cleaning industrial optics and spectacle lenses
  • Impregnated cleaning wipes for surfaces requiring mild solvent action
  • Process carriers for silicone oils, greases, and selected industrial formulations
Product Family

DOWSIL OS-30

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Boiling Point
194 °C
Flash Point
57 °C
General Properties
Specific Gravity
0.85
Surface Tension
17.3 mN/m
Vapor Pressure
0.43 mmHg

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of DOWSIL™ OS-30 Fluid. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Flash point, closed cup 57 (135) °C (°F) Closed cup
Boiling point 194 (381) °C (°F) At 760 mm Hg
Vapor pressure 0.43 mm Hg At 25°C (77°F)
Drying rate 0.14 — Butyl acetate = 1; ASTM D-1901
Viscosity 1.3 cP At 25°C (77°F)
Specific gravity 0.85 — At 25°C (77°F)
Surface tension 17.3 dynes/cm At 25°C (77°F)
Freezing point -68 (-90) °C (°F) Typical value

Leading Brands Trust in Our Products and Services