DOWSIL HC 1000 Silicone Adhesive

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL HC 1000 Silicone Adhesive

Main features

  • One-Part, Solventless Silicone Coating
  • Room-Temperature Adhesive Cure
  • 21 kV/mm Dielectric Strength

Product Description

DOWSIL™ HC 1000 Gray Conformal Coating is a one-part, solventless polydimethylsiloxane conformal coating developed for environmental and dielectric protection of printed circuit board assemblies. The high-viscosity material cures through exposure to atmospheric moisture at room temperature and reaches a typical tack-free state in 11 minutes at 25°C. After cure, it forms a soft, low-stress silicone elastomer that helps protect assemblies exposed to moisture, vibration and harsh operating environments. Its gray pigmentation can hinder component identification, while controlled volatility supports use around sensitive electronic devices. The coating also carries a UL 94 V-0 flammability classification.

Key features

  • Solventless, one-part formulation: Supplied as a ready-to-use silicone coating with 97.6% typical non-volatile content.
  • Soft, low-stress cured elastomer: Typical Shore A hardness of 24 supports stress-relieving protection of delicate components and interconnections.
  • Controlled volatility and flame classification: Designed for use around sensitive devices and classified UL 94 V-0.

Applications / Suitable for

  • Printed circuit board system assemblies
  • Appliances requiring dielectric insulation
  • Electronic assemblies requiring protection from moisture, vibration and harsh operating environments
Product Family

DOWSIL HC 1000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Gray
Component System
One
Specific Gravity
1.07
Physical Properties
Tack-Free Time
11 minutes
Viscosity
12,000 mPa.s
Electrical Properties
Dielectric Strength
21 kV/mm
Volume Resistivity
2.0 E15 Ohms⋅cm
Thermal Properties
UL 94 Rating
94 V0

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of DOWSIL™ HC 1000 Gray Conformal Coating in its as-supplied condition. Values are not intended for preparing specifications.

Property Value Unit Method / condition
Components One — As supplied
Color Gray — Typical
Viscosity 12,000 cP (mPa·s) Typical
Non-volatile content 97.6 % Typical
Tack-free time 11 minutes Room-temperature cure at 25°C
Room-temperature cure time 0.5 hours Cure time depends on application method, film thickness, temperature and humidity
Technical properties

After-processing / final-state properties

Typical properties of the cured coating. Values are not intended for preparing specifications or for use alone as design values.

Property Value Unit Method / condition
Specific gravity 1.07 — Cured
Durometer hardness 24 Shore A Cured
Dielectric strength 525 (21) V/mil (kV/mm) JIS K 6249
Volume resistivity 2.0 × 1015 ohm·cm JIS K 6249
Dielectric constant 3.2 — At 1 MHz
Dissipation factor 0.003 — JIS K 6249; at 1 MHz
Flammability classification V-0 — UL 94