DOWSIL EA-9189 H

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL EA9189-H

Main features

  • One-Part No-Mix Bonding
  • Tack-Free Time at 25 deg C
  • UL 94 V-0 Classification

Product Description

DOWSIL™ EA-9189 H White RTV Adhesive is a one-part, moisture-curing silicone adhesive for module assembly applications. The alkoxy-cure RTV formulation requires no mixing and develops a tack-free surface in approximately 2 minutes at 25°C, supporting short handling intervals during assembly. After cure, the white adhesive combines a Shore A hardness of 80 with documented adhesion to aluminum, copper, polycarbonate, and FR-4 test substrates. It also provides thermal conductivity of 0.88 W/m·K, high volume resistivity, dielectric strength of 28 kV/mm, and a UL 94 V-0 flammability classification for electronics assembly applications requiring mechanical attachment, electrical insulation, and flame-rated material performance.

Key features

  • One-part moisture cure: The ready-to-use alkoxy-cure formulation requires no component mixing and cures at room temperature.
  • Fast tack-free time: Forms a tack-free surface in approximately 2 minutes at 25°C.
  • Electrical and flame performance: Provides 3.3 × 1015 ohm·cm volume resistivity, 28 kV/mm dielectric strength, and a UL 94 V-0 classification after cure.

Applications / Suitable for

  • Module assembly
  • Battery-pack assemblies
  • Electronic boards, components, and housings
Product Family

DOWSIL EA-9189 H

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Specific Gravity
1.68
Physical Properties
Tack-Free Time
2 minutes
Mechanical Properties
Elongation
32 %
Thermal Properties
Thermal Conductivity
0.88 W/m.K
UL 94 Rating
94 V-0
Electrical Properties
Dielectric Strength
28 kV/mm
Volume Resistivity
3.3E15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Representative product characteristics before cure.

Property Value Unit Method / condition
Component count One-part — As supplied
Physical form Paste — As supplied
Color White — Visual
Cure system Alkoxy moisture cure — Room-temperature cure
Tack-free time 2 minutes 25°C

After-processing / final-state properties

Typical cured-material properties. Values are not intended for use as product specifications.

Property Value Unit Method / condition
Specific gravity 1.68 — Cured material
Tensile strength 3.9 MPa Equivalent to 576 psi
Elongation 32 % Cured material
Hardness 80 Shore A Durometer
Thermal conductivity 0.88 W/m·K Cured material
Volume resistivity 3.3 × 1015 ohm·cm Cured material
Dielectric strength 28 kV/mm Equivalent to 700 V/mil
Flammability classification UL 94 V-0 — Cured material