DOWSIL CC-2588

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL CC-2588

Main features

  • Five-Minute Tack-Free Processing
  • 22.3 kV/mm Dielectric Strength
  • Firm Abrasion-Resistant Cure

Product Description

DOWSIL CC-2588 Conformal Coating applies as a one-part, transparent, medium-viscosity silicone resin coating for rigid and flexible circuit boards. The colorless-to-pale-yellow liquid has a typical Brookfield viscosity of 930 cP, 88% nonvolatile content and a five-minute tack-free time at 25 deg C and 50% relative humidity. After cure, it forms a firm, abrasion-resistant surface with Shore A 75 hardness, 22.3 kV/mm dielectric strength and 5.04 MPa tensile strength. Spray, brush, flow, dip and automated pattern coating are supported, with solvent flash-off and cure conditions controlled for the applied film thickness.

Key features

  • Five-minute tack-free time: Supports rapid room-temperature handling at 25 deg C and 50% relative humidity.
  • High-solids application: Typical nonvolatile content is 88%.
  • Firm dielectric coating: Cured hardness is Shore A 75 with 22.3 kV/mm dielectric strength.

Applications

Protective conformal coating of rigid and flexible circuit boards and printed wiring boards.

Product Family

DOWSIL CC-2588

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Colorless to pale yellow liquid
Specific Gravity
1.06 / 1.11
Physical Properties
Viscosity
930 mPa.s
Mechanical Properties
Elongation
233 %
Electrical Properties
Dielectric Strength
22.3 kV/mm
Volume Resistivity
2.4E15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and process properties. Values are not specifications.

Property Value Unit Method / condition
Component count One-part As supplied
Color Colorless to pale yellow liquid CTM0176
Viscosity 930 cP CTM0050; Brookfield LV, spindle #2 at 10 rpm
Specific gravity 1.06 Uncured; CTM0097
Tack-free time 5 min At 25 deg C and 50% RH; CTM0098
Nonvolatile content 88 % CTM0208; forced-draft volatility
Typical cure schedule 10 min RT + 10 min at 60 deg C 3 mil (75 um) coating after solvent flash-off
Technical properties

After-processing / final-state properties

Typical cured coating properties. Values are not specifications.

Property Value Unit Method / condition
Specific gravity 1.11 Cured; CTM0540
Durometer hardness 75 Shore A CTM0099
Dielectric strength 22.3 kV/mm CTM0114
Tensile strength 5.04 MPa CTM0137A
Elongation 233 % CTM0137A
Volume resistivity 2.4E15 ohm cm CTM0249
Glass transition temperature -117 deg C DMA
Coefficient of thermal expansion 180 ppm CTM0563