DOWSIL 995

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL 995

Main features

  • 350 psi Ultimate Tensile Strength
  • +/-50% Structural Joint Movement
  • 10-20-Minute Structural Glazing Window

Product Description

DOWSIL 995 Silicone Structural Sealant supports structural bonding of glass and metal and protective glazing with a one-part, neutral-cure silicone formulation. The ready-to-use material provides a 10-20 minute working time, 65-minute tack-free time and seven- to fourteen-day cure at 25 deg C and 50% relative humidity. After seven days, it reaches Shore A 40 hardness, 350 psi ultimate tensile strength and 525% elongation. Structural-glazing installations require project-specific joint design, substrate testing, quality controls and specific Dow approval; the product data do not replace system-level engineering validation.

Key features

  • High ultimate tensile strength: Typical seven-day ultimate tensile strength is 350 psi.
  • 10-20 minute working time: Supports placement and tooling before surface cure.
  • +/- 50% joint movement: ASTM C719 movement capability applies after 21 days of cure.

Applications

Structural bonding of glass and metal and protective glazing within project-specific Dow design and approval controls.

Product Family

DOWSIL 995

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black, gray, white
Specific Gravity
1.339
Physical Properties
Tack-Free Time
65 minutes
Mechanical Properties
Elongation
525 %
Peel Strength
40 ppi

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and cure-development properties. Values are not specifications.

Property Value Unit Method / condition
Color Black, gray or white As supplied
Tack-free time 65 min ASTM C679; 50% RH
Curing time 7-14 days At 25 deg C and 50% RH
Full adhesion 14-21 days Typical value
Flow, sag or slump 0.1 in ASTM C639
Working time 10-20 min Typical value
Specific gravity 1.339 As supplied
VOC content 30 g/L SCAQMD basis
Technical properties

After-processing / final-state properties

Typical cured properties at 25 deg C and 50% relative humidity. Seven-day and 21-day values are identified separately.

Property Value Unit Method / condition
Durometer hardness 40 Shore A After seven days; ASTM D2240
Ultimate tensile strength 350 (2.41) psi (MPa) After seven days; ASTM D412
Ultimate elongation 525 % After seven days
Tear strength, Die B 49 ppi After seven days; ASTM D624
Peel strength 40 ppi After seven days; ASTM C794
Tensile at 25% elongation 43 (0.30) psi (MPa) After 21 days; ASTM C1135
Tensile at 50% elongation 65 (0.43) psi (MPa) After 21 days; ASTM C1135
Joint movement capability +/- 50 % After 21 days; ASTM C719