DOWSIL 93-006-6

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

DOWSIL 93-006-6

Main features

  • Long Working-Time Assembly
  • High-Viscosity Non-Sag Placement
  • Two-Part Ambient Cure

Product Description

DOWSIL 93-006-6 RF Aerospace Sealant is a two-part, high-viscosity, non-sag silicone elastomer sealant for high-performance aerospace sealing applications. The base and catalyst are mixed before application and cure at room temperature to form a flexible silicone rubber. Its long working window and controlled extrusion behavior support placement on prepared, primed surfaces where bead stability and assembly time are important. Surface preparation, component proportioning, mixing and room-temperature cure conditions must be controlled for the application. Aerospace use remains limited to the exact process and qualification scope established for the specific assembly.

Key features

  • Two-part room-temperature cure: Supports controlled mixing and ambient cure processing.
  • High-viscosity non-sag handling: Maintains bead placement on prepared surfaces.
  • Aerospace sealing format: Applies to high-performance sealing within the qualified assembly scope.

Applications

High-performance aerospace sealing and bonding or sealing to properly prepared, primed surfaces.

Product Family

DOWSIL 93-006-6

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two (base / Catalyst)
Mix Ratio
10:1
Mechanical Properties
Elongation
170 %
Peel Strength
325 psi

Additional Information

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers