Product Description

DOWSIL 795 Silicone Building Sealant serves structural and nonstructural glazing, panel attachment and weathersealing with a one-part, neutral-cure silicone formulation. The non-sag material provides a 20-30 minute working time, three-hour tack-free time and seven- to fourteen-day cure at 25 deg C and 50% relative humidity. After 21 days, the sealant has Shore A 35 hardness, 32 lb/in peel strength and +/- 50% joint movement capability. Structural applications require a properly designed joint, substrate testing, installation controls and prior approval by the local Dow sales application engineer.

Key features

  • Structural and weatherseal versatility: One material is used for glazing, panel attachment and weathersealing.
  • 20-30 minute working time: Supports application and tooling before surface cure.
  • +/- 50% joint movement: ASTM C719 movement capability applies after 21 days of cure.

Applications

Structural and nonstructural glazing, panel attachment, stiffener bonding and weathersealing within project-specific design controls.

Technical Specifications

Physical Properties
Tack-Free Time
180 minutes
Mechanical Properties
Peel Strength
5.7 kg/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical application and cure-development properties. Values are not specifications.

Property Value Unit Method / condition
Tack-free time 3 hr ASTM C679; 50% relative humidity
Curing time 7-14 days At 25 deg C and 50% RH
Full adhesion 14-21 days Typical cured joint
Flow, sag or slump 0.1 (2.54) in (mm) ASTM C639
Working time 20-30 min Typical value
VOC content 30 g/L SCAQMD basis
Technical properties

After-processing / final-state properties

Typical properties after 21 days at 25 deg C and 50% relative humidity unless noted.

Property Value Unit Method / condition
Durometer hardness 35 Shore A ASTM D2240
Peel strength 32 (5.7) lb/in (kg/cm) ASTM C794
Tension adhesion at 25% extension 45 (0.310) psi (MPa) ASTM C1135
Tension adhesion at 50% extension 60 (0.) psi (MPa) ASTM C1135
Joint movement capability +/- 50 % ASTM C719
Staining None ASTM C1248; granite, marble, limestone, brick and concrete
Tension adhesion after QUV, 25% extension 35 (0.241) psi (MPa) ASTM C1135; after 10000 hr QUV
Tension adhesion after QUV, 50% extension 50 (0.345) psi (MPa) ASTM C1135; after 10000 hr QUV