DOWSIL 790

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

DOWSIL 790

Main features

  • +100/-50% Joint Movement
  • Ultra-Low-Modulus Cured Seal
  • Non-Sag 10-20-Minute Tooling

Product Description

DOWSIL 790 Silicone Building Sealant provides one-part, neutral-cure, ultra-low-modulus sealing for new and remedial construction joints. Its non-sag formulation provides a 10-20 minute working time and a one-hour tack-free time at 50% relative humidity, supporting vertical and overhead joint installation. After seven days at 25 deg C and 50% relative humidity, the sealant has Shore A 15 hardness and ASTM C719 +100/-50% extension/compression capability for high-movement joints. Applications include expansion and control joints, precast concrete panel joints, EIFS joints, curtain-wall and mullion joints, and stone-paver joints. The product is not intended for structural applications.

Key features

  • Ultra-low-modulus cure: Shore A 15 hardness supports high-movement construction joints.
  • Class 100/50 movement: ASTM C719 extension/compression capability is +100/-50%.
  • Non-sag application: A 10-20 minute working time supports tooling before cure.

Applications

Expansion, control, precast-panel, EIFS, curtain-wall, mullion and stone-paver movement joints.

Technical Specifications

Physical Properties
Tack-Free Time
60 minutes
Mechanical Properties
Peel Strength
4.46 kg/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical application and cure-development properties. Values are not specifications.

Property Value Unit Method / condition
Tack-free time 1 hr ASTM C679; 50% relative humidity
Curing time 7-14 days At 25 deg C and 50% RH; 3/8 in depth
Full adhesion 14-21 days Cured joint
Flow, sag or slump None ASTM D2202
Working time 10-20 min CTM 98
VOC content, maximum 23 g/L EPA Method 24
Technical properties

After-processing / final-state properties

Typical properties after seven days at 25 deg C and 50% relative humidity.

Property Value Unit Method / condition
Durometer hardness 15 Shore A ASTM C661
Tensile strength, maximum 100 psi ASTM D412
Peel strength 25 lb/in ASTM C794
Tensile at 25% extension 15 psi ASTM C1135
Tensile at 50% extension 20 psi ASTM C1135
Joint movement capability +100/-50 % ASTM C719; extension/compression
Staining None ASTM C1248; various substrates