DOWSIL 7500

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

DOWSIL 7500

Main features

  • Color-Coded 1:1 Mixing
  • Five-Minute 125 deg C Cure
  • Stencil-Printable Electronics Bonding

Product Description

DOWSIL 7500 Adhesive Kit uses color-coded two-part components and a 1:1 mix ratio to create a translucent green, heat-cure silicone pressure-sensitive adhesive for electronics assembly. Part A is translucent yellow and Part B is translucent blue, helping confirm component loading and mixing. The material is stencil- or screen-printable and cures in five minutes at 125 deg C to a soft pressure-sensitive elastomer for bonding electronic components, FR4, heat sinks and module parts. Complex-viscosity values at defined shear rates and a thixotropic ratio of 2.3 support process evaluation, while the cured adhesive has Shore 00 hardness and 90-degree peel data.

Key features

  • Color-coded 1:1 mixing: Yellow and blue components produce a green mixed adhesive for visual verification.
  • Five-minute heat cure: Typical cure time is five minutes at 125 deg C.
  • Stencil and screen printability: Rheology supports patterned electronics-assembly application.

Applications

Pressure-sensitive bonding of electronic components, FR4, heat sinks and module components.

Product Family

DOWSIL 7500

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent yellow / Translucent blue
Component System
Two (A /B)
Physical Properties
Thixotropic index
2.3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material and process values. Values are not specifications.

Property Value Unit Method / condition
Mix ratio 1:1 Part A to Part B
Component appearance Translucent yellow / translucent blue Part A / Part B
Mixed appearance Translucent green After correct mixing
Part A / Part B complex viscosity 100000 / 80000 cP CTM1098; 10 rad/sec
Mixed complex viscosity 81000 / 35500 cP CTM1098; 10 / 100 rad/sec
Thixotropic ratio 2.3 CTM1098
Heat-cure time 5 min At 125 deg C
Shelf life 12 months At 25 deg C
Technical properties

After-processing / final-state properties

Typical properties of the heat-cured pressure-sensitive adhesive. Cure condition is five minutes at 125 deg C unless otherwise stated.

Property Value Unit Method / condition
Cured form Soft pressure-sensitive elastomer Heat-cured mixed adhesive
Durometer hardness 40 Shore 00 CTM0099
90-degree peel adhesion 2.4 lb/in CTM0270

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers