DOWSIL 730 FS SOLVENT RESISTANT SEALANT

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL 730 FS SOLVENT RESISTANT SEALANT

Main features

  • One-Component Sealing System
  • Room-Temperature Sealing Cure
  • Non-Sag Placement Control

Product Description

DOWSIL™ 730 FS Solvent Resistant Sealant is a one-component, solventless fluorosilicone adhesive/sealant supplied as a non-sag paste. The acetoxy-cure material reacts with atmospheric moisture at room temperature to form a tough, flexible rubber that retains its properties when exposed to fuels, oils, and solvents. Its paste consistency supports application on vertical and overhead surfaces, while the cured material remains stable and flexible across a documented temperature range of -65°C (-85°F) to 260°C (500°F). It is used for bonding, sealing, caulking, and formed-in-place gasketing where fluid exposure and demanding environmental conditions must be considered.

Key features

  • Fuel, oil, and solvent resistance: Retains its properties under exposure to fuels, oils, and solvents and resists fluid-related swelling.
  • One-component moisture cure: Ready-to-use acetoxy system cures at room temperature when exposed to moisture in the air.
  • Non-sag paste consistency: Supports application on vertical and overhead surfaces without slumping or running.

Applications / Suitable for

  • Bonding and sealing where resistance to fuels, oils, and solvents is required
  • Assembly and repair of fuel systems and tanks
  • Formed-in-place gaskets for irregular shapes and harsh service conditions
  • Components exposed to moisture, vibration, shock, fuels, oils, and solvents
Product Family

DOWSIL 730 FS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
white
Specific Gravity
1.44
Physical Properties
Extrusion Rate
321 g/min
Skin Time
12 minutes
Tack-Free Time
14 minutes
Mechanical Properties
Elongation
195 %
Electrical Properties
Arc Resistance
124 s
Dielectric Strength
14.6 kV/mm
Volume Resistivity
5.1x10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the material as supplied. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance Non-slump paste — CTM 0176
Color White — As supplied
Extrusion rate 321 g/minute CTM 0364; 3.2 mm orifice at 0.62 MPa (1/8 in orifice at 90 psi)
Skin-over time 12 minutes CTM 0098
Tack-free time 14 minutes CTM 0095
Technical properties

After-processing / final-state properties

Typical mechanical properties after curing for 7 days in air at 23°C (73°F) and 50% relative humidity. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Specific gravity 1.44 — CTM 0022 / ASTM D792
Durometer hardness 40 Shore A CTM 0099 / ASTM D2240
Tensile strength 3.0 (434) MPa (psi) CTM 0137A / ASTM D412
Elongation at break 195 % CTM 0137A / ASTM D412
Tear strength 11.9 (68) kN/m (ppi) CTM 0159A / ASTM D624, die B
Peel strength 6.8 (39) kN/m (ppi) CTM 0293; primed aluminum

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers