DOWSIL™ 710 Fluid is a polyphenylmethylsiloxane fluid for high-temperature lubrication and heat-transfer applications. It retains its properties during continuous use at temperatures up to 260° C in closed systems and combines low volatility with resistance to oxidation and gumming. The fluid is suitable for lubricating timing devices, instruments, and bearings operating from 0 to 260 °C. It may also be used as a base oil for high-temperature greases thickened with molybdenum disulphide and as a heat-exchange fluid in high-temperature baths and metal heat-treating baths.

Key features

  • High-temperature stability: Retains its properties during continuous use at temperatures up to 260 °C in closed systems.
  • Low volatility: Shows 3.0% volatility after four hours at 250 °C and has negligible vapor pressure at 25 °C.
  • Oxidation and radiation resistance: Resists oxidation and gumming and remains serviceable after radiation doses of up to 200 megarads at room temperature.

Applications / Suitable for

  • Timing devices, instruments, and bearings operating from 0 to 260 °C
  • Base oil for high-temperature greases thickened with molybdenum disulphide
  • High-temperature heat-exchange baths
  • Metal heat-treating baths
Product Family

DOWSIL 710

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Colorless to light straw
Refractive index
1.533
Specific Gravity
1.11
Surface Tension
28.5 mN/m
Thermal Properties
Flash Point
302 °C
Thermal Conductivity
0.14 W/m.K
Electrical Properties
Dielectric Strength
14 kV/mm
Volume Resistivity
1E13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of DOWSIL™ 710 Fluid. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color Colorless to light straw — As supplied
Viscosity 500 mm²/s At 25°C
Specific gravity 1.11 — At 25°C/15.6°C
Flash point 302 °C Open cup
Volatility 3.0 % After 4 hours at 250°C
Vapor pressure Negligible kPa At 25°C
Vapor pressure 0.01 kPa At 149°C
Vapor pressure 0.2 kPa At 232°C
Vapor pressure 0.5 kPa At 260°C
Vapor pressure 1.3 kPa At 288°C
Vapor pressure 2.9 kPa At 316°C
Vapor pressure 11.0 kPa At 371°C
Thermal decomposition point 370 °C Typical value
Spontaneous ignition temperature 488 °C Typical value
Freeze point -22 °C Typical value
Coefficient of expansion 0.00072 1/°C From 0°C to 135°C
Sound velocity 1370 m/s At 25°C
Compressibility 1.70 % At 34.5 MPa
Compressibility 3.15 % At 69 MPa
Compressibility 5.50 % At 138 MPa
Thermal conductivity 0.14 W/(m·K) At 50°C
Specific heat 1.52 kJ/(kg·K) At 40°C
Specific heat 1.64 kJ/(kg·K) At 100°C
Specific heat 1.84 kJ/(kg·K) At 200°C
Molecular weight, average 2600 — Average value
Refractive index 1.533 — At 25°C
Surface tension 28.5 mN/m At 25°C
Electric strength 14 kV/mm 2.5 mm gap; rapid rise
Permittivity 2.95 — At 25°C and 100 Hz
Permittivity 2.95 — At 25°C and 100 kHz
Dissipation factor 0.002 — At 25°C and 100 Hz
Dissipation factor 0.0002 — At 25°C and 100 kHz
Volume resistivity 1 × 1013 ohm·cm Typical value