DOWSIL 3-6548

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

DOWSIL 3-6548

Main features

  • Fire-Resistant RTV Silicone Foam
  • 2x to 4x Liquid-Volume Expansion
  • Flexible Medium-Density Ozone/UV-Resistant Foam

Product Description

DOWSIL™ 3-6548 RTV Foam Kit is a two-part, room-temperature-vulcanizing silicone foam primarily used in fire-resistant penetration-seal and linear-joint systems. It expands to approximately two to four times its liquid volume and cures into a flexible, medium-density elastomeric foam, allowing it to fill irregular openings and difficult-to-reach spaces. The product is formulated to withstand high temperatures and confine smoke, flames, and gases in supported building-system configurations. Its expanding, electrically insulating silicone foam structure also supports use in electronics applications where flexible filling, cushioning, insulation, or environmental protection is required. Part A and Part B are mixed at a 1:1 ratio by weight or volume.

Key features

  • Fire-resistant sealing: Primarily positioned for specified penetration-seal and linear-joint systems that restrict the passage of smoke, flames, and gases.
  • Expanding RTV foam: Expands to approximately two to four times its liquid volume and cures at room temperature to fill complex or difficult-to-access spaces.
  • Flexible insulating foam: Forms a medium-density silicone foam with approximately 50% closed cells and documented dielectric properties for building and electronics applications.

Applications / Suitable for

  • Fire-resistant penetration-seal systems
  • Linear floor and floor-to-wall joints
  • Sealing irregular openings against smoke, flames, gases, and contaminants
  • Electronics applications requiring flexible filling, cushioning, insulation, or environmental protection
Product Family

DOWSIL 3-6548

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Compression Pressure
0.71 Kg/cm2
Density
300 kg/m3
Thermal Properties
Thermal Conductivity
0.075 W/m.K
Electrical Properties
Dielectric Strength
6.6 kV/mm
Volume Resistivity
2.25E15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the separate liquid components and properly mixed material. These values are not intended for preparing specifications.

Property Value Unit Method / condition
Appearance — Part A Black liquid — CTM 0176
Appearance — Part B Off-white liquid — CTM 0176
Specific gravity — Parts A and B 1.05–1.11 — CTM 0097; 25°C (77°F)
Viscosity — Part A 40–60 poise CTM 0050; Brookfield HAF, spindle No. 3 at 10 rpm
Viscosity — Part B 50–75 poise CTM 0050; Brookfield HAF, spindle No. 3 at 10 rpm
Mix ratio 1:1 — Part A to Part B, by weight or volume
Snap time / working time 1–2 minutes Properly mixed material at 25°C (77°F); time to non-pour condition and beginning of foam rise

After-processing / final-state properties

Typical properties after mixing one part A with one part B and curing at 25°C (77°F) for 24 hours, unless otherwise stated. Results may vary with cured foam density.

Property Value Unit Method / condition
Appearance Dark gray-black elastomeric foam — CTM 0176
Free-foam density 0.22–0.32 g/cm³ CTM 0812; power mixed for 30 seconds and cured unconfined
Closed-cell content 50 % CTM 0826; breathability method
Tensile strength 2.28 × 105 N/m² ASTM D 3574; equivalent to 33.0 psi
Compression deflection at 40% compression 6.96 × 104 N/m² CTM 0525; equivalent to 10.1 psi
Thermal conductivity 0.1338 W/(m·K) ASTM C 518; 2.54 cm-thick foam sample, density reported as 0.27 g/cm³
Linear coefficient of thermal expansion 3.2 × 10−4 cm/cm·°C CTM 0585; −25 to 150°C
Dielectric strength 165 V/mil CTM 0114; cured foam sample thickness 0.317 cm (0.125 inch)