DowSil 3-6077 RTV Silicone Ablative

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DowSil 3-6077 RTV Silicone Ablative

Main features

  • 0.035 mm/s Ablation Penetration Rate
  • 2 to 3-Hour Working Window
  • Spray or Trowel Application

Product Description

DOWSIL™ 3-6077 RTV Silicone Ablative is a two-part, non-slumping silicone elastomer developed for aerospace ablative protection. The room-temperature-curing system can be sprayed or trowelled for use as an ablative coating, thermal barrier, high-temperature pressurization sealant, or rocket liner. It combines low thermal conductivity with flexibility across temperature extremes and forms a moderately tough char that can be removed after exposure to support surface cleaning and recoating.

Key features

  • Ablative thermal protection: Provides a documented penetration rate of 0.035 mm/s under an oxy-acetylene torch exposure of 45 W/cm².
  • Room-temperature cure: Uses a 10:1 base-to-catalyst mix ratio by weight and cures in 24 hours at 25 °C.
  • Flexible application: Non-slumping material can be sprayed, trowelled, applied with a spatula, or dispensed from a pressure gun.

Applications / Suitable for

  • Protection of launch structures exposed to direct rocket blast
  • Ablative coatings and thermal barriers
  • High-temperature pressurization seals
  • Rocket liner applications
Product Family

DOWSIL 3-6077

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
white/blue
Density
1.58 kg/m3
Mix Ratio
10:1
Physical Properties
Viscosity
1,9000,000 mPa.s
Mechanical Properties
Elongation
50 %
Thermal Properties
Thermal Conductivity
0.29 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and processing properties of DOWSIL™ 3-6077 RTV Silicone Ablative. Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Product form Two-part, non-slumping silicone elastomer — As supplied
Consistency Viscous liquid — As supplied
Color White base / blue catalyst — As supplied
Base viscosity 1,900,000 mPa·s CTM 0050 / ASTM D1084; at 25 °C
Mixing ratio 10 base : 1 catalyst by weight Catalyzed mixture
Relative density 1.58 — CTM 0022; mixed 10:1 by weight at 25 °C
Working time 2–3 hours After catalyst addition at approximately 25 °C
Cure time 24 hours At 25 °C
Usable life 12 months Original unopened containers stored at or below 32 °C

 

Technical properties

After-processing / final-state properties

Typical cured properties of DOWSIL™ 3-6077 RTV Silicone Ablative after seven days at room temperature, except where otherwise noted. Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Tensile strength 4.2 MPa CTM 0137A / ASTM D412; cured 7 days at room temperature
Elongation at break 50 % CTM 0137A / ASTM D412; cured 7 days at room temperature
Durometer hardness 73 Shore A CTM 0099 / ASTM D2240; cured 7 days at room temperature
Deep-section cure Yes — 25 mm thickness
Thermal conductivity 0.29 W/(m·K) Cured material; test method not stated
Specific heat 1.04 kJ/(kg·K) At 25 °C; test method not stated
Ablation penetration rate 0.035 mm/s Oxy-acetylene torch exposure at 45 W/cm²
Char retention Fair — Oxy-acetylene torch exposure at 45 W/cm²

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers