DOWSIL™ 3-1944 HP RTV Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL™ 3-1944HP RTV Coating

Main features

  • One-Part, Solventless Silicone Coating
  • 7-Minute Tack-Free Time
  • Integrated UV Indicator

Product Description

DOWSIL™ 3-1944 HP RTV Coating is a one-part, translucent polydimethylsiloxane coating for localized protection and thin-section encapsulation in electronic assemblies. The solventless material cures through exposure to atmospheric moisture at room temperature, with optional mild heat acceleration at temperatures up to 60°C. Its 53,000 mPa·s viscosity supports controlled flow and needle dispensing, while the cured coating forms a soft, low-stress elastomer. An integrated UV indicator supports visual or automated inspection, and the coating carries a UL 94 V-0 flammability classification under UL 746C.

Key features

  • One-part moisture cure: Requires no mixing and cures at room temperature through exposure to atmospheric moisture, with optional mild heat acceleration.
  • Soft, low-stress elastomer: Cures to a translucent silicone elastomer with a typical hardness of 36 Shore A.
  • UV inspection and flame resistance: Contains a UV indicator for visual or automated inspection and is classified UL 94 V-0 under UL 746C.

Applications / Suitable for

  • Pin and solder-joint coverage
  • Thin-section encapsulation
  • Spot protection of pins and other devices
Product Family

DOWSIL 3-1944 HP

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
translucent
Component System
one part
Specific Gravity
1
Physical Properties
Tack-Free Time
7 minutes
Viscosity
53,000 mPa.s
Thermal Properties
UL 94 Rating
V-0

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and processing properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Number of components One — As supplied; no mixing required
Appearance Translucent — CTM 0176
Viscosity 53,000 cP CTM 0050; equivalent to 53,000 mPa·s or 53 Pa·s
Tack-free time 7 minutes CTM 0098; at 25°C; tack-free time does not indicate full cure
Shelf life 12 months At 25°C; observe the Use Before date on the product label and protect opened material from moisture
Technical properties

After-processing / final-state properties

Typical cured-material properties and product-specific flammability classification. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Specific gravity 1 — CTM 0097; cured material
Hardness 36 Shore A CTM 0099; cured material
Flammability classification 94 V-0 — UL 746C; recognition is subject to applicable coating-thickness and substrate requirements