PEAM-1769 Difunctional (meth)acrylate

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

PEAM-1769 Difunctional (meth)acrylate

Main features

  • Ultra low modulus
  • Thermal stability
  • High adhesion to various substrates

Product Description

PEAM-1769 is a polyester acrylate/methacrylate that exhibits excellent adhesion, low warpage, and hydrophobicity. The oligomer has very high thermal stability and low volatility. It can be used as a base oligomer in a formulation or an additive. It is dark amber-colored, something that needs to be considered for light cure application.

PEAM-1769 is recommended for use as a base resin or an additive to reduce stress. It has excellent adhesion on most substrates with low stress and low shrinkage due to its high Tg polycyclic repeat units. The oligomer has good solubility in both aliphatic and aromatic solvents and monomers.

Product Family

DMI PEAM-1769

1. Select Package Type
Price starting from €209.04
Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber liquid
Functionality
2
Molecular weight
1769 g/mol
Thermal Properties
Decomposition Temperature
>375 °C
Glass Transition Temperature (Tg)
-40 °C
Weight Loss @ 300°C
3.0 %
Other Properties
Storage Temperature
10 °C
Physical Properties
Viscosity
20000 mPa.s