MM304 | Methacrylate adhesion promoter Additive
Harmonization Code : 2925.19.95.90 | Carboxyimide-function compounds (including saccharin and its salts) and imine-function compounds : Imides and their derivatives; salts thereof : Other : Other : Other
Main features
- Mild pleasant odor
- Hydrolytic resistance
- Lower weight loss on cure than IBOMA
Product Description
MM-304 is a liquid mono-functional methacrylate monomer. It has similar properties as Isobornyl Methacrylate (IBOMA) when polymerized but with lower weight loss on cure. It has a mild, pleasant odor. MM-304 has good resistance to hydrolysis.
MM-304 is recommended as a reactive diluent monomer for use in UV or peroxide cure formulations. It is particularly recommended for applications that require hydrolytic resistance.
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Colorless
Density (g)
0.96 g/cm3
Molecular weight
304 g/mol
Refractive index
1.5
Thermal Properties
Flash Point
>175 °C
Other Properties
Storage Temperature
5 °C
Physical Properties
Viscosity
80 mPa.s