A675-100 | PMDGM adhesion promoter Additive

Harmonization Code : 3824999390 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included Other:

A675-100 | PMDGM adhesion promoter Additive

Main features

  • Versatile
  • Adhesion promoter
  • Pyromellitic Dianhydride Glycerol Dimethacrylate Adduct

Product Description

A-675-100% is a versatile additive for adhesion enhancement, provided as a neat viscous liquid. The four methacrylate groups and two carboxylic groups per molecule allow bonding to a variety surfaces.

A-675-100% is recommended for use as an adhesion enhancing additive. The PMDGM abbreviation stands for Bis(Glyceryl Dimethacrylate) Pyromellitate or Pyromellitic Dianhydride Glycerol Dimethacrylate Adduct. It is TSCA listed.

Product Family

DMI A675-100

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Light Yellow liquid
Molecular weight
674.603 g/mol