A1100 | Anti bleed Additive

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

A1100 | Anti bleed Additive

Main features

  • 0.5%-1% wt
  • Metal surfaces
  • Excellent bleed control

Product Description

A-1100 is a proprietary non-halogenated additive designed to reduce resin bleed out on a variety of surfaces with minimal or no affect on the adhesion properties of the formulation. It shows excellent results when used in non-metal filled systems after reducing bleed. It is co-curable in free-radical polymerization. It also can enhance the rheological properties of various filled adhesives.

A-1100 is recommended for use as an additive to reduce resin bleed out specifically on metal surfaces and has more acid functionality per molecule then A-1050. The recommended addition of the A-1100 to a formulation is between 0.5% - 1% weight percent of resin. It shows superior bleed control in formulations that contain non-metal fillers such as silica.

Product Family

DMI A1100

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Yellow liquid
Density (g)
1.01 g/cm3
Functionality
2 Functional group/molecule
Molecular weight
1226 (Estimated) g/mol
Thermal Properties
Flash Point
146 °C
Physical Properties
Viscosity
475 mPa.s

Additional Information

Epoxy Resin Incompatibility

A1100 rely on acid functionality to bond in and prevent bleeding. Unfortunately thiol group react with epoxy resin instead of substrate reducing or even eliminating the resin bleed functionality.

 

Molecular Weight Estimation

We do not specifically measure the M.W. for this material and instead rely on the average M.W. of the starting material and the functionality (thiol group) that makes the product.