DK15EG-05 Black Insulating Coating Powder

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Electrostatic DK15EG-05 Black Insulating Coating Powder DK15EG-05 Black Insulating Coating Powder DK15EG-05 Black Insulating Coating Powder DK15EG-05 Black Insulating Coating Powder DK15EG-05 Black Insulating Coating Powder

Main features

  • DK15EG-05 Coating Powder
  • Black, insulating, epoxy based
  • Gasohol resistant, for automotive fuel pump motor armatures

Product Description

DK15EG-05 Black is an epoxy based coating powder developed for the insulation of motor armatures and stators. It offers cut-through temperature resistance and is flex-fuel (unleaded gasoline and methanol) resistant. DK15EG-05 Black is designed to be applied by an electrostatic fluid bed process, offering a fast cure in an induction coil curing process. Particle size is tailored to provide low dusting levels.

DK15EG-05 is flex-fuel (gasohol, gasoline/ethanol blend) resistant, Class F-rated epoxy powder coating for slot insulation of automotive fuel pump motor armatures and stators. It works extremely well for both AC and DC electric motors, including those used for in-tank fuel pumps. The coating provides superior flex fuel resistance, edge coverage, and high impact strength. High cut through temperature serves to protect the motor even at high operating temperatures. DK15EG-05 is designed for electrostatic fluid bed application, and DK15EG-05 is tested and qualified for UL EIS 1446 155°C (Class F) rating.

DK15EG-05 is available in both black and green color. It is black in color, though DK15EG-05 Green is the green color version of DK15EG-05 Black.  Both versions have been used for over 20 years by major manufacturers of automotive enclosures, fuel pumps, windshield wipers, seat adjusters, and other, DK15EG-05 provides a smooth surface appearance with high edge coverage. Particle size is optimized for high productivity on an electrostatic fluidized bed coating process including Braun Sondermaschinen.

Advantages of DK15EG-05 for Slot Insulation

  • Flex-fuel resistant, suitable for exposure to automotive fluids
  • A high pickup powder, it provides high productivity on Braun Sondermaschinen and other electrostatic fluidized bed machines
  • Permits the use of more copper in the slots allowing for smaller, higher-power motors
  • Reduced copper waste compared to slot liners since the winding does not need to go up and over the liner
  • Excellent moisture resistance, even in high temperatures and corrosive conditions
  • A high-productivity coating powder, used for decades in the manufacture of fuel pump assemblies

Typical applications and uses of DK15EG-05 Black or Green include:

  • Slot Insulation of AC and DC Motor Armatures
  • Slot Insulation of Stators
  • Slot Insulation of Motor Armatures in Fuel Pump Motors
  • It has also been tested successfully for hairpin coating of 400V electric motors

This product is no longer available. Some alternatives for armature and stator coating powders are:

MCP-5260 Class F Motor Coating Powder

MCP-5000 Class B Motor Coating Powder

Product Family

DK0942

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Epoxy
Color
Black
Density (g)
0.74/0.67 g/cm3
Process Method
Epoxy Coating Powders
Specific Gravity
1.75
Thermal Properties
Glass Plate Flow
22/20 mm
UL 94 Rating
Class B (130°C)
Electrical Properties
Cut Through Temperature
345 °C
Dielectric Strength
1010 kV/mm
Other Properties
Certifications
ESF-M3L72-A
RoHS Compliant
Yes
Special Properties
Gasohol Resistant
Mechanical Properties
Edge Coverage
40 %

Additional Information

{tab=Pricing & Availability}

Pricing for {product_name}

Pricing and Volume Price Breaks for {product_name} are available by contacting us. You cannot order this product directly online.

KRAYDEN lists all its prices without taxes, shipping payment charges or discounts. KRAYDEN has warehouses and ships from both Canada and the Netherlands, and if your shipping address is one of these two countries, applicable taxes will be applied. If your shipping address is to the United States, we request your company’s Employer Identification Number (EIN) or Tax Identification Number (TIN). This is a unique 9-digit number assigned by the IRS and is required for all cross-border shipments. Failure to provide this number could result in delays to your order. If your shipping address is within the EU, but outside the Netherlands, then we are required to request your company's Value Added Tax (VAT, BTW, MwSt) number to be able to ship the goods tax-free. For all other countries, no taxes are levied on your orders.

Minimum Order Quantity for {product_name}

The minimum order quantity for this package size is {min_order_quantity} {product_unit}(s).

Shipping Charges for {product_name}

All prices shown are ex-works KRAYDEN, but during the checkout process, you will be given several shipping options including Canada Post, TNT, UPS or the choice of using your own freight forwarder. Depending on your shipping address, the shipping charges will be calculated as follows:

  • Europe, Middle East, Asia and Africa: Shipping from KRAYDEN Europe BV (Amsterdam, the Netherlands)
  • Canada, USA, Mexico and South America: Shipping from KRAYDEN Corporation (Ottawa, Canada)

Payment option for {product_name}

During the checkout process, you will be presented with several payment options including:

  • Credit Card (We accept VISA and Mastercard)
  • Bank Transfer (You will be given the payment instructions at the time of order placement)
  • PayPal (Where you can also pay with American Express Cards)
  • Purchase Order (You must be preapproved first. See our Online Credit Application)

Availability for {product_name}

To the right of the product is a small icon that lets you know the availability and leadtime of the product. This leadtime is the time to ship the product and delivery times vary based on the method of delivery you select at the time you place your order. Contact us if anything is unclear or you need more assistance.

{tab=Technical Specifications}

Short Description of {product_name}

Technical Datasheets for {product_name}

TDS (English) Kapton_Technical_Data_Sheet Click to access {product_name} Technical Data Sheet
*Note that only registered users may access technical datasheets

{tab=Competitive Crossovers}

#shortdesc

Compare price and quality of DK15-0907 Red Insulating Epoxy Coating Powder to these other brands

Please see the section above for a list of Competitive Brands that {product_name} competes against.

{tab=Videos & Other Media}

Videos & Other Related Media

Please visit or subscribe to our YouTube Channel.

See this video that shows the difference between a good and a bad fluidized epoxy coating powder bed.

{tab=Product Reviews}

Product Reviews for {product_name}

{review}

{tab=Packaging Details}

Packaging Details for {product_name}

The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to to approximate delivery charges using your own carrier.

Each unit of {product_name} has the following:

  • Unit of Measurement: {product_unit}
  • Dimensions (length x width x height): {length} x {width} x {height} {lwh_uom}
  • Weight: {weight} {weight_uom}

{tab=View Blogs & Forum}

Read and discuss {product_name} on KRAYDEN's Blog and Forum
KRAYDEN is different. Unlike other business to business enterprises, we encourage our customers to discuss, critique, and otherwise comment on the products we offer. Get more technical information, read detailed posts, and see what customers have to say about about {product_name} on our Corporate Blog and Forum.
  • Read more about {product_name} on our Blog.
  • Join the discussion about {product_name} on our Forum.

{/tabs}

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers