DK15-0463 Black Insulating Epoxy Coating Powder

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Black busbar epoxy coating for low voltage on copper DK15-0463 Black Insulating Epoxy Coating Powder DK15-0463 UL94-V0 listed and recognized Fine grind version of DK15-0463 for better fluidized epoxy beds Low voltage busbar epoxy coating powder on aluminum Moisture resistant epoxy coating powder for low voltage outdoor

Main features

  • DK15-0463 Coating Powder
  • Black, insulating, epoxy based
  • Humidity-resistant for outdoor low voltage busbars

Product Description

DK15-0463 is an epoxy-based coating powder developed for the insulation of low-voltage busbars. It offers improved moisture resistance and dielectric strength along with a smooth surface appearance. The particle size distribution is optimized for use in large fluid bed coating operations. DK15-0463 has a UL Relative Thermal Index (RTI) rating of 130°C, making it ideal for applications requiring high thermal stability. Used for over 20 years by major power distribution companies for low-voltage outdoor bus bar applications, DK15-0463 provides a reliable coating with high edge coverage. The fusion bonded coating is smooth, tough, and moisture-resistant for applications up to 600V. DK15-0463 is UL recognized Particle size is optimized for the fluidized bed coating process.

Advantages of DK15-0463 for Busbar Coating

  • Excellent bed life—so important for large busbar coating operations
  • Excellent moisture resistance, even in high temperatures and corrosive conditions
  • Suitable for both copper and aluminum busbar coating
  • Smooth surface allows closer bar spacing in busway
  • An extremely reliable coating powder, used for decades in the power distribution industry

Typical applications and uses of DK15-0463 Black include:

  • Low Voltage (600V) Copper, Aluminum and Brass Busbars
  • Outdoor busbar applications
  • Switchgear Equipment for Power Distribution

This product is no longer available. Some alternatives for busbar coating powders are:

Product Family

DK0463

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Plate Flow
27 mm
UL 94 Rating
V-0
Electrical Properties
Dielectric Strength
44 kV/mm
Volume Resistivity
8.6x10^16 Ohms⋅cm
Other Properties
RoHS Compliant
yes
Special Properties
Halogen - Free
Mechanical Properties
Edge Coverage
45 %
General Properties
Chemistry Type
Powder
Color
Black
Density (g)
0.69 g/cm3
Specific Gravity
1.52