DEVCON SF5MIN

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DEVCON SF5MIN

Main features

  • Fast Five-Minute Metal Repair
  • Non-Sag Vertical Rebuilding
  • Machinable Steel-Filled Repairs

Product Description

Devcon Plastic Steel 5-Minute Putty (SF) is a two-component, steel-filled epoxy putty for filling, rebuilding, and bonding metal surfaces. Its putty consistency can be troweled up to 1/4 in (6.4 mm) thick on vertical surfaces without sagging, while a 5-minute pot life at 75 deg F supports rapid repair work. The material reaches functional cure in 1 hour and full cure in 16 hours at room temperature, after which it can be machined, drilled, or painted. Applications include restoring worn metal, patching castings, making jigs and fixtures, and rebuilding pump or valve bodies.

Key features

  • Five-minute working window: The mixed putty has a 5-minute pot life at 75 deg F for rapid repair work.
  • Non-sag vertical repairs: The material can be troweled up to 1/4 in (6.4 mm) thick on vertical surfaces.
  • Machinable steel-filled finish: After full cure, the repair can be machined, drilled, or painted.

Applications / Suitable for

  • Restoring worn or fatigued metal
  • Patching castings and rebuilding pump or valve bodies
  • Making jigs, fixtures, and bearing-journal repairs
Product Family

DEVCON SF5MIN

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Dark Grey
Component System
Two Part
Pot Life
5 minutes
Specific Gravity
2.2
Electrical Properties
Dielectric Strength
1.2 kV/mm
Thermal Properties
Temperature Resistance
93 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and mixed properties at 72-75 deg F (23-24 deg C) unless noted.

Property Value Unit Method / condition
Color Dark gray Uncured material
Mix ratio by volume 1:1 Resin to hardener
Mix ratio by weight 1.7:1 Resin to hardener
Mixed viscosity Putty At 72 deg F (23 deg C)
Pot life 5 min At 75 deg F
Specific gravity 2.2 At 72 deg F (23 deg C)
Specific volume 12.2 (0.44) in3/lb (cm^3/g) At 72 deg F (23 deg C)
Technical properties

After-processing / final-state properties

Typical cured properties after 7 days at 75 deg F (24 deg C); values are not specifications.

Property Value Unit Method / condition
Adhesive tensile shear 2,026 (14.0) psi (MPa) ASTM D1002; cured 7 days at 75 deg F (24 deg C)
Compressive strength 10,400 (71.7) psi (MPa) ASTM D695; cured 7 days at 75 deg F (24 deg C)
Flexural strength 7,680 (52.9) psi (MPa) ASTM D790; cured 7 days at 75 deg F (24 deg C)
Hardness 85 Shore D ASTM D2240; cured 7 days at 75 deg F (24 deg C)
Cured shrinkage 0.0006 in/in ASTM D2566; cured 7 days at 75 deg F (24 deg C)
Coefficient of thermal expansion 34 (61.2) x 10^-6 in/in deg F (cm/cm deg C) ASTM D696; cured 7 days at 75 deg F (24 deg C)
Dielectric strength 30 (1.2) V/mil (kV/mm) ASTM D149; cured 7 days at 75 deg F (24 deg C)
Dry temperature resistance 200 (93) deg F (deg C) Cured material