Devcon® 10 Minute™ Epoxy is a rapid-curing, two-part epoxy adhesive and encapsulant for industrial bonding applications. The 100%-solids, solvent-free system bonds metals, fabrics, ceramics, glass, wood, and concrete in compatible combinations. It features a 1:1 mix ratio by volume or weight, a 10-minute working time, and a functional cure in 1.5 hours at room temperature. Available in black and clear versions, it provides rigid cured performance with documented mechanical and electrical properties.

Key features

  • Rapid-curing epoxy system: Provides a 10-minute working time, 20-minute fixture time, and 1.5-hour functional cure.
  • Convenient 1:1 mixing: Resin and hardener mix at a 1:1 ratio by either volume or weight.
  • Multi-material bonding: Bonds metals, fabrics, ceramics, glass, wood, and concrete in compatible combinations.

Applications / Suitable for

  • General-purpose industrial bonding
  • Encapsulation of industrial components
  • Bonding compatible combinations of metals, fabrics, ceramics, glass, wood, and concrete
Product Family

DEVCON 10 MINUTE EPOXY

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
black or clear
Density
1,130 kg/m3
Mix Ratio
1:1
Solids
100 %
Mechanical Properties
Elongation
5 %
Electrical Properties
Dielectric Strength
31.5 kV/mm
Thermal Properties
Operating Temperature
-40°C - 93° °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and processing properties of Devcon® 10 Minute™ Epoxy at 72 °F (23 °C), except where otherwise noted. Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Color Black or clear — Uncured at 72 °F (23 °C)
Mix ratio 1:1 — By volume or weight
Mixed viscosity 80,000–90,000 cP Uncured at 72 °F (23 °C)
Mixed density 9.4 (1.13) lb/gal (g/cm³) Uncured at 72 °F (23 °C)
Working time 10 minutes Uncured at 72 °F (23 °C)
Fixture time 20 minutes Uncured at 72 °F (23 °C)
Functional cure 1.5 hours At 72 °F (23 °C)
Full cure 12 hours At 72 °F (23 °C)
Solids by volume 100 % Typical

 

Technical properties

After-processing / final-state properties

Typical cured properties of Devcon® 10 Minute™ Epoxy after seven days at 75 °F (24 °C). Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Adhesive lap shear 2,400 (16.55) psi (MPa) ASTM D1002; cured 7 days at 75 °F (24 °C)
Hardness 75 Shore D ASTM D2240; cured 7 days at 75 °F (24 °C)
Dielectric strength 800 (31.5) V/mil (kV/mm) ASTM D149; cured 7 days at 75 °F (24 °C)
Impact resistance 10 (21) ft-lb/in² (kJ/m²) Cured 7 days at 75 °F (24 °C); test method not stated
Tensile elongation 5 % Cured 7 days at 75 °F (24 °C); test method not stated
T-peel strength 20–25 (3.5–4.4) pli (N/mm) Cured 7 days at 75 °F (24 °C); test method not stated
Service temperature -40 to 200 (-40 to 93) °F (°C) Documented service-temperature range