CYBERBOND 2999

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2999

Main features

  • Surface-Insensitive Porous-Material Bonding
  • Thixotropic Vertical-Surface Control
  • High-Viscosity Gap Filling

Product Description

Cyberbond CB 2999 is a one-part, surface-insensitive ethyl cyanoacrylate gel for fast bonding on acidic and porous materials as well as common engineering substrates. Its thixotropic, very high-viscosity profile keeps the adhesive in place on vertical surfaces and supports gap filling without the flow behavior of lower-viscosity grades. The colorless, transparent adhesive has cone-and-plate viscosity of 35,000 to 60,000 cP at 0.5 rpm and 3,000 to 6,000 cP at 160 rpm at 20 deg C. Setting-time data are provided for steel, EPDM, ABS, and beech wood.

Key features

  • Surface-insensitive fast bonding: The ethyl cyanoacrylate bonds acidic and porous materials including wood, leather, cardboard, and paper.
  • Thixotropic vertical control: The gel remains in place on vertical surfaces during application.
  • Very high-viscosity gap filling: The rheology supports gap-filling bonds where a low-flow adhesive is required.

Applications / Suitable for

  • Bonding wood, leather, cardboard, and paper
  • Vertical-surface cyanoacrylate bonding
  • Gap-filling bonds on supported substrates
Product Family

CYBERBOND 2999

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
colorless, transparent
Density (g)
1.08 g/cm3
Thermal Properties
Flash Point
80 °C
Other Properties
Storage Temperature
20 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured monomer properties at 20 deg C unless noted; values are not specifications.

Property Value Unit Method / condition
Base compound Ethyl-2-cyanoacrylate Uncured monomer
Appearance Colorless, transparent Uncured monomer
Density 1.08 g/cm^3 20 deg C
Flash point 80 deg C Uncured monomer
Shelf life 12 months Unopened at 20 deg C
Viscosity 35,000-60,000 cP Cone-and-plate, 0.5 rpm at 20 deg C
Viscosity 3,000-6,000 cP Cone-and-plate, 160 rpm at 20 deg C
Technical properties

After-processing / final-state properties

Cured polymer and bonded-substrate properties under the stated stated conditions.

Property Value Unit Method / condition
Cured polymer appearance Transparent Polymer
Service temperature range -55 to 95 deg C Cured polymer
Bond strength on NBR rubber 5-12 N/mm^2 Cured adhesive; material failure indicated
Bond strength on steel 8-17 N/mm^2 Cured adhesive