CYBERBOND 2241

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2241

Main features

  • Toughened Structural Bonding
  • Metal, Plastic, and Rubber Bonding
  • Up to 140 deg C Service

Product Description

CYBERBOND 2241 is a black, fast-setting, rubber-toughened ethyl cyanoacrylate adhesive from the xtraflex Series. Designed as a partly flexible adhesive, it provides shock absorbence and high temperature resistance, making it excellent for dynamic, temperature-loaded bonds and combination bonding of metals to rubber or plastics.

Key features

  • Rubber toughened: Offers partial flexibility to absorb shocks and withstand dynamic loads.
  • High temperature resistance: Maintains performance across a broad service temperature range of -55 to 140°C.
  • Fast bonding performance: Features quick setting times, such as 6-16 seconds on EPDM and 7-13 seconds on ABS plastics.

Applications / Suitable for

  • Combination bonding of metal to rubber.
  • Combination bonding of metal to plastic.
  • Applications requiring shock absorbence and dynamic load resistance.
Product Family

CYBERBOND 2241

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Specific Gravity
1.06 g/cm³
Physical Properties
Viscosity
2,000 to 4,000 (Uncured Monomer) mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Uncured monomer properties of CYBERBOND 2241.

Property Value Unit Method / condition
Base Compound Ethyl-2-cyanoacrylate - -
Appearance Black - -
Density 1.06 g/cm³ at 20°C
Viscosity 2000-4000 cps cone-plate, @ 20°C @ 160 rpm
Setting Time (Metal/Steel) 30-90 seconds -
Setting Time (EPDM) 6-16 seconds -
Setting Time (Plastic/ABS) 7-13 seconds -
Technical properties

After-processing / final-state properties

Physical properties of cured CYBERBOND 2241 polymer.

Property Value Unit Method / condition
Service Temperature Range -55 to 140 °C -
Strength (Steel) 18 to 28 N/mm² -
Strength (NBR-rubber) 5 to 12 N/mm² Material failure