CYBERBOND 2077

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2077

Main features

  • Medium-Viscosity Placement Control
  • Fast Rubber-Compound Bonding
  • Metal, Plastic, and Rubber Fit

Product Description

Cyberbond 2077 provides a medium-viscosity ethyl cyanoacrylate option for fast general-purpose bonding, particularly rubber compounds. The intermediate flow profile balances placement control with wetting on close-fitting metal, plastic, and rubber interfaces. It is applied without mixing and develops rapid set under substrate-specific conditions, supporting small-part assembly. Cyberbond 2077 offers a medium-body instant adhesive for joints that need controlled placement without a high-viscosity gap-filling profile, especially in rubber-focused applications and controlled small-part assembly workflows.

Key features

  • Medium-viscosity placement control: The flow profile balances wetting with localized application on close-fitting parts.
  • Rubber-compound bonding: The adhesive is particularly used for rubber and elastomer assemblies.
  • Substrate-specific fast set: Set behavior is reported for metal, plastic, and rubber interfaces.

Applications / Suitable for

  • Rubber and elastomer bonding
  • Close-fitting metal and plastic parts
  • General-purpose small-component assembly
Product Family

CYBERBOND 2077

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear
Density (g)
1.06 g/cm3
Thermal Properties
Flash Point
85 °C
Physical Properties
Viscosity
800 +/- 150 mPa.s
Other Properties
RoHS Compliant
Yes
Storage Temperature
15.5 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values. Values are not specifications.

Property Value Unit Method / condition
Technology / base Ethyl Cyanoacrylate
Components One component Ready-to-use liquid
Cure initiation Humidity Cyanoacrylate cure mechanism
Appearance / consistency Clear liquid As supplied
Viscosity 800 +/- 150 cP Typical product value
Specific gravity 1.06 Typical product value
Flash point 85 deg C 185 deg F
Shelf life 12 months Unopened original container; store 15.5 to 25 deg C

Leading Brands Trust in Our Products and Services