CYBERBOND 2075

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2075

Main features

  • High-Viscosity Gap-Filling Bonding
  • Controlled Joint Placement
  • Single-Component Fast Assembly

Product Description

Cyberbond 2075 uses a medium- to high-viscosity ethyl cyanoacrylate format for general-purpose bonding where gap filling and controlled placement are needed. Its thicker consistency helps keep adhesive at the joint rather than relying on wicking flow, supporting less closely fitted parts and localized application. The product cures without premixing and supports fast assembly of compatible substrates. Cyberbond 2075 provides a higher-body instant adhesive option for small gaps and bond areas where added material body is useful.

Key features

  • Higher-viscosity gap filling: The adhesive is used where small gaps require more body than a wicking cyanoacrylate.
  • Controlled joint placement: The thicker liquid profile supports localized application at the bond area.
  • Single-component fast bonding: The one-part adhesive supports rapid assembly without a mix step.

Applications / Suitable for

  • General-purpose bonding with small gaps
  • Less closely fitted component joints
  • Localized adhesive placement and rapid assembly
Product Family

CYBERBOND 2075

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear
Density (g)
1.06 g/cm3
Thermal Properties
Flash Point
85 °C
Physical Properties
Viscosity
550 +/- 150 mPa.s
Other Properties
Storage Temperature
15.5 to 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and application characteristics for the one-component adhesive. Values are not specifications.

Property Value Unit Method / condition
Technology / base Ethyl cyanoacrylate One-component adhesive
Physical form Medium- to high-viscosity liquid As supplied
Cure mechanism Humidity initiated Cyanoacrylate cure
Application behavior Controlled localized placement Reduced wicking compared with low-viscosity grades
Gap behavior Small-gap filling Close-fitting bonded assemblies