CYBERBOND 2010

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2010

Main features

  • 20-Second General-Purpose Fixture
  • Controlled Low-Viscosity Application
  • 2,920 psi Stainless-Steel Shear

Product Description

Cyberbond 2010 is a one-component, solvent-free ethyl cyanoacrylate adhesive for fast general-purpose bonding. It has a typical viscosity of 95 to 200 mPa s at 20 deg C and fixtures in about 20 seconds, supporting controlled application to metals, elastomers, rubber, and plastics. Substrate-specific set times range from 2 to 4 seconds on ABS to 5 to 40 seconds on steel under the stated conditions. The cured adhesive provides a 2,920 psi shear strength on stainless steel and a service temperature range of -55 to 95 deg C.

Key features

  • Fast general-purpose fixture: Typical fixture time is 20 seconds, with substrate-specific set times reported for ABS, EPDM, steel, and beech.
  • Controlled low-viscosity flow: Typical viscosity is 95 to 200 mPa s at 20 deg C using a cone-plate method.
  • Stainless-steel bond strength: Reported cured shear strength is 2,920 psi on stainless steel.

Applications / Suitable for

  • Metal and stainless-steel bonding
  • Elastomer, rubber, and EPDM assemblies
  • Plastic and ABS component bonding
Product Family

CYBERBOND 2010

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear
Density (g)
1.06 g/cm3
Thermal Properties
Flash Point
85 °C
Physical Properties
Viscosity
110 +/- 20 mPa.s
Other Properties
Storage Temperature
15.5 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical product and process values. Values are not specifications.

Property Value Unit Method / condition
Physical form Liquid As supplied
Viscosity 95 to 200 mPa s 20 deg C, 158 s^-1, cone-plate method
Density 1.06 g/cm^3 Typical value
Fixture time 20 seconds Typical value
Flash point 82.5 deg C Uncured product