COOTHERM CIRCALOK 6037

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

COOTHERM CIRCALOK 6037

Main features

  • Thermally Conductive Bonding
  • 500,000 cP Resin Viscosity
  • 1.2 W/(m K) Thermal Conductivity

Product Description

CoolTherm® EP-6037 Epoxy Resin is a thermally conductive epoxy resin formulated for use with selected CoolTherm hardeners to create two-component bonding systems. The black or green paste is used in semiconductor and electronics assemblies to form thermally conductive joints in fabricated heat sinks, between heat sinks and power devices, and between semiconductors or transistors and heat sinks. The resin has a typical viscosity of 500,000 cP at 25°C and a specific gravity of 2.35. Processing and final properties depend on whether CoolTherm EP-6010 or EP-6252 hardener is selected.

Key features

  • Thermally conductive epoxy resin: The resin is paired with selected CoolTherm hardeners for heat-sink and power-device bonding.
  • Controlled paste consistency: Typical resin viscosity is 500,000 cP at 25°C.
  • Two documented hardener options: EP-6010 and EP-6252 provide different mix ratios and cured-property profiles.

Applications / Suitable for

  • Thermally conductive joints in fabricated heat sinks
  • Bonding heat sinks to power devices
  • Bonding semiconductors and transistors to heat sinks
Product Family

COOTHERM 6037

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black or Green Paste
Specific Gravity
2.35
Physical Properties
Viscosity
500,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Appearance Black or green paste N/A As supplied
Viscosity 500,000 cP At 25°C
Specific gravity 2.35 N/A As supplied
Mix ratio with EP-6010 100:3.4 parts by weight Resin : hardener
Working life with EP-6010 2 h At 25°C
Mix ratio with EP-6252 100:7.1 parts by weight Resin : hardener
Working life with EP-6252 3 h At 25°C
Cure options 24 h at 25°C; 2 h at 65°C N/A Both documented hardener systems
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Thermal conductivity 1.2 W/m·K With EP-6010; ISO 22007-2 Hot Disc
CTE 52 ppm/°C With EP-6010
Glass-transition temperature 106 °C With EP-6010; TMA
Hardness 93 Shore D With EP-6010
Thermal conductivity 1.1 W/m·K With EP-6252; ISO 22007-2 Hot Disc
CTE 31 ppm/°C With EP-6252
Glass-transition temperature 70 °C With EP-6252; TMA
Hardness 92 Shore D With EP-6252