COOLTHERM SC-6731

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6731

Main features

  • 100 cP Resin Viscosity
  • Concentrations from 0.1% to 5% by Weight
  • Two-Component RTV Silicone Systems Used in Potting

Product Description

CoolTherm™ SC-6731 Hardener is a low-viscosity curing agent for use with compatible CoolTherm™ and Circalok™ silicone resins to form two-component, room-temperature-vulcanizing silicone systems for potting and encapsulation. The light amber, translucent liquid has a typical viscosity of 100 cP at 25°C and may be used at concentrations from 0.1% to 5% by weight, depending on the selected resin and required cure rate. Product-specific mixing ratios, working times, and cure schedules must be taken from the applicable silicone resin datasheet.

Key features

  • Low viscosity: Provides a typical viscosity of 100 cP at 25°C for incorporation into compatible silicone resin systems.
  • Adjustable concentration: May be used at 0.1% to 5% by weight, depending on the cure rate required and the applicable resin formulation.
  • Silicone-system versatility: Designed for use with various CoolTherm and Circalok silicone resins used in RTV potting and encapsulation systems.

Applications / Suitable for

  • Compatible CoolTherm and Circalok RTV silicone resin systems
  • Two-component silicone potting and encapsulation systems
Product Family

COOLTHERM SC-6731

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Light Amber Translucent Liq
Specific Gravity
1.1
Physical Properties
Viscosity
100 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties and documented use concentration for CoolTherm SC-6731 Hardener. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Light amber, translucent liquid — As supplied
Viscosity 100 cP At 25°C; test method not stated
Specific gravity 1.1 — Test conditions and method not stated
Use concentration 0.1–5 wt% Depending on required cure rate; use the applicable resin datasheet for the specific mix ratio
Shelf life 6 months From date of manufacture when stored at 25°C in the original, unopened container