CoolTherm™ SC-6730 Hardener is a high-viscosity catalyst for use with RTV condensation-cure silicone resins when fast room-temperature cure in thick sections is required. The blue-green liquid supports visual confirmation of thorough mixing and may be used at concentrations from 3.0% to 10.0% by weight, depending on the cure rate required. It cures deep sections without exotherm and provides documented resistance to copper corrosion. Specific mix ratios, application instructions, and cure schedules depend on the selected resin system.

Key features

  • Deep-section cure: Supports room-temperature curing in thick sections without exotherm.
  • Adjustable catalyst concentration: May be used at 3.0% to 10.0% by weight, depending on the cure rate required.
  • Visible mixing indicator: Its blue-green color supports visual examination of mixing uniformity.

Applications / Suitable for

  • RTV condensation-cure silicone resin systems
  • Thick-section silicone curing requiring fast room-temperature cure
Product Family

COOLTHERM SC-6730

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue Green Liq
Specific Gravity
1.44
Physical Properties
Viscosity
5000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties and documented use concentration for CoolTherm SC-6730 Hardener. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Blue-green liquid — As supplied
Viscosity 5,000 cP At 25°C; test method not stated
Specific gravity 1.44 — Test conditions not stated
Use concentration 3.0–10.0 wt% Depending on required cure rate; use the applicable resin datasheet for the specific mix ratio
Shelf life 6 months From date of manufacture when stored at 25°C in the original, unopened container