COOLTHERM SC-6714

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6714

Main features

  • UL 94 V-0 Encapsulation
  • 55 to 205 deg C Service Range
  • Circalok 6730/6731 Catalyst Compatibility

Product Description

Circalok™ 6714 is a two-component silicone potting compound that cures at room temperature or elevated temperature to produce a non-burning, thermally conductive elastomeric rubber. The material provides excellent electrical insulation and environmental protection for encapsulated assemblies. It is listed by UL as non-burning in accordance with UL 94 V-0 and is recommended for applications requiring thermal conductivity, electrical performance, and durable environmental sealing. :contentReference[oaicite:0]{index=0}

Key Features

  • Thermally conductive silicone: Produces a thermally conductive elastomer suitable for heat-generating electronic assemblies. :contentReference[oaicite:1]{index=1}
  • UL 94 V-0 listed: Documented as non-burning in accordance with UL 94 V-0. :contentReference[oaicite:2]{index=2}
  • Flexible processing: Cures at room temperature or elevated temperature and is compatible with Circalok™ 6731 or Circalok™ 6730 catalysts. :contentReference[oaicite:3]{index=3}

Applications / Suitable for

  • Electronic potting requiring environmental protection
  • Applications requiring thermal conductivity
  • Applications requiring non-burning encapsulation
Product Family

COOLTHERM SC-6714

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Specific Gravity
1.36
Physical Properties
Viscosity
15000 mPa.s
Thermal Properties
Thermal Conductivity
0.68 W/m.K
Electrical Properties
Volume Resistivity
10^14 Ohms⋅cm

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical uncured properties of Circalok™ 6714. Values are not intended for specification purposes. :contentReference[oaicite:4]{index=4}

Property Value Unit Method / Condition
Appearance White — Standard color
Specific Gravity 1.36 g/cc 25°C
Viscosity 15,000 cP 25°C
Shelf Life 6 months From date of manufacture
Compatible Catalysts Circalok™ 6731 or Circalok™ 6730 — Per handling instructions
Technical Properties

After-Processing / Final-State Properties

Typical cured properties of Circalok™ 6714. Values are not intended for specification purposes. :contentReference[oaicite:5]{index=5}

Property Value Unit Method / Condition
Tensile Strength 700 psi 25°C
Elongation 130 % At yield
Linear Shrinkage 0.003 in/in —
Service Temperature -55 to 205 (continuous)
-100 to 300 (intermittent)
°C Service conditions
Hardness 45 Shore A —
Thermal Conductivity 4.7 BTU/ft²/hr/°F/in Typical value
Coefficient of Thermal Expansion 15 × 10⁻⁵ in/in/°C —
Volume Resistivity 10¹⁴ ohm-cm 25°C
Dielectric Constant 5.0 — 25°C, 100 kHz
Dissipation Factor 0.015 — 25°C, 100 kHz
Dielectric Strength 450–500 V/mil —

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers