COOLTHERM SC-6709

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6709

Main features

  • 1.0 W/(m K) Thermal Encapsulation
  • Three Hardener Options
  • 68 to 205 deg C Service Range

Product Description

CoolTherm® SC-6709 Silicone Encapsulant is a two-component, solvent-free RTV silicone system for thermally conductive potting and encapsulation. The white SC-6709 resin may be combined with CoolTherm SC-6731, CoolTherm SC-6730, or Circalok™ 6732 hardener to provide different mix ratios and room-temperature cure times. After cure, the flexible silicone provides typical thermal conductivity of 1.0 W/m·K, dielectric strength of 21.7 kV/mm, and a documented operating-temperature range from -68°C to +205°C.

Key features

  • Thermally conductive encapsulation: Provides typical cured thermal conductivity of 1.0 W/m·K using the Hot Disc Transient Method, ISO 22007-2.
  • Multiple hardener options: Compatible with CoolTherm SC-6731, CoolTherm SC-6730, and Circalok 6732 hardeners for configurable mix ratios and cure times.
  • Broad operating-temperature range: Suitable for parts and devices experiencing temperatures from -68°C to +205°C.

Applications / Suitable for

  • Thermally conductive potting and encapsulation
  • Applications requiring flexible silicone encapsulation and high-temperature service
Product Family

COOLTHERM SC-6709

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White Liquid
Specific Gravity
1.80
Physical Properties
Viscosity
32000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm SC-6709 resin and its supported resin-to-hardener systems before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance White liquid — CoolTherm SC-6709 resin as supplied
Viscosity 32,000 cP CoolTherm SC-6709 resin at 25°C; test method not stated
Specific gravity 1.80 — CoolTherm SC-6709 resin at 25°C
Mix ratio by weight 100:0.5 / 100:5 or 100:10 / 100:0.5 Resin:hardener SC-6731 / SC-6730 / Circalok 6732 hardener, respectively
Gel time 1–2 / 0.5–1 / 2–3 hours At 25°C with SC-6731 / SC-6730 / Circalok 6732 hardener, respectively; both SC-6730 mix ratios have the same stated range
Cure time 12–16 / 8–12 / 6–8 hours At 25°C with SC-6731 / SC-6730 / Circalok 6732 hardener, respectively; both SC-6730 mix ratios have the same stated range
Shelf life 6 months CoolTherm SC-6709 resin stored at 25°C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm SC-6709 silicone systems. The cured properties are stated to be the same regardless of the supported hardener used. Values are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 1.0 W/m·K Hot Disc Transient Method, ISO 22007-2
Coefficient of linear thermal expansion 50 ppm/°C Test method and temperature region not stated
Hardness 50 Shore A Test method not stated
Tensile strength 2.14 (310) MPa (psi) At 25°C; test method not stated
Elongation at break 115 % Test method and test temperature not stated
Moisture absorption 0.08 % 10 days at 25°C; exposure medium and test method not stated
Volume resistivity 1 × 1015 ohm-cm At 25°C; test method not stated
Dielectric strength 21.7 (550) kV/mm (V/mil) ASTM D149; specimen thickness not stated

Leading Brands Trust in Our Products and Services