COOLTHERM EP 6972 KIT

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

COOLTHERM EP 6972 KIT

Main features

  • <0.0005 ohm-cm Volume Resistivity
  • 2.13 W/(m K) Thermal Conductivity
  • 1:1 Weight Mixing

Product Description

CoolTherm EP-6972 Conductive Adhesive is a two-part, silver-filled epoxy adhesive for electrically and thermally conductive bonding. Resin and hardener mix 1:1 by weight for manual or automatic meter/mix/dispense application. Cure schedules are 40 minutes at 85 deg C or 20 minutes at 100 deg C after the material reaches the target temperature. Typical cured properties include volume resistivity below 0.0005 ohm-cm and thermal conductivity of 2.13 W/(m K). The stated service-temperature range is -50 to +150 deg C.

Key features

  • Cured volume resistivity: Typical cured value is below 0.0005 ohm-cm at 25 deg C using ASTM D257.
  • Cured thermal conductivity: Typical cured thermal conductivity is 2.13 W/(m K).
  • Equal-ratio weight mixing: Resin and hardener mix 1:1 by weight before application.

Applications

General circuit board repair; conductive bonding where electrical and thermal conductivity are required.

Product Family

COOLTHERM EP-6972

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Silver Paste
Component System
Two (Resin / Hardener)
Specific Gravity
3.49 / 3.55

Additional Information

Technical properties

As-supplied / before-processing properties

Resin and hardener are supplied as separate components; mixed values apply after the 1:1 by-weight mix.

PropertyValueUnitMethod / condition
Mix ratio, resin:hardener1:1by weightBefore application
Specific gravity, resin3.49Typical; resin
Specific gravity, hardener3.55Typical; hardener
Specific gravity, mixed3.52Typical; mixed material
Working life>1hTypical; mixed material; 25 deg C; 100 g mass
Technical properties

Cured adhesive properties

PropertyValueUnitMethod / condition
Volume resistivity<0.0005ohm-cmTypical; ASTM D257; 25 deg C
Thermal conductivity2.13W/(m K)Typical
Hardness80Shore DTypical
Lap shear strength1200psiTypical; aluminum-to-aluminum