COOLTHERM EP-6010

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-6010

Main features

  • 55 cP Application Viscosity
  • Low-Shrinkage Epoxy Curing Agent
  • Two-Year Shelf Life at 25 deg C

Product Description

CoolTherm® EP-6010 Hardener is an amber liquid epoxy curing agent designed for use with various CoolTherm® and LORD® epoxy resins. When combined with an applicable resin, it creates a two-component system for electrical encapsulation and bonding applications. The hardener is formulated to support low shrinkage and reduced stress on components during cure while producing a rigid, resilient final system.

Key Features

  • Low-stress curing: Exhibits low shrinkage and stress on components as the epoxy system cures.
  • Rigid cured system: Produces a rigid system with documented resilience when used with an applicable epoxy resin.
  • Low viscosity: Provides a typical viscosity of 55 cP at 25°C.

Applications / Suitable for

  • Two-component electrical encapsulation systems
  • Two-component epoxy bonding systems
Product Family

COOLTHERM EP-6010

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber Liquid
Specific Gravity
0.92
Physical Properties
Viscosity
55 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm EP-6010 Hardener as supplied. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Amber liquid — As supplied
Viscosity 55 cP At 25°C; test method not stated
Specific gravity 0.92 — Test method and temperature not stated
Shelf life 2 years From date of manufacture when stored in a cool, dry environment at 25°C in the original, unopened container