COOLTHERM EP-3500

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-3500

Main features

  • 3.3 W/(m K) Thermal Conductivity
  • 10.4 to 12 ppm/deg C CTE
  • 205 to 206 deg C Glass Transition

Product Description

CoolTherm® EP-3500 Epoxy Resin is a dark gray, highly filled epoxy resin formulated for use with CoolTherm® EP-3500 Hardener or CoolTherm® EP-2000 Hardener. The two-component systems are designed for encapsulating motor stators, transformer coils, and electrical devices requiring a rigid material with high thermal conductivity and a low coefficient of linear thermal expansion. Depending on the selected hardener, the cured system provides a typical thermal conductivity of 2.6 or 3.3 W/m·K, a glass transition temperature of approximately 205–206 °C by TMA, and electrical insulation properties.

Key features

  • High thermal conductivity: Provides a typical cured thermal conductivity of 3.3 W/m·K with EP-3500 Hardener or 2.6 W/m·K with EP-2000 Hardener.
  • Low thermal expansion: Delivers a typical coefficient of linear thermal expansion of 10.4–12 ppm/°C, depending on the selected hardener.
  • High-temperature cured system: Provides a typical glass transition temperature of 205–206 °C by TMA.

Applications / Suitable for

  • Motor stator encapsulation
  • Transformer-coil encapsulation
  • Electrical devices requiring rigid, thermally conductive encapsulation with low thermal expansion
Product Family

COOLTHERM EP-3500

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Drak Gray Paste
Specific Gravity
2.98
Physical Properties
Viscosity
@ 60°C 10/s 9200 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
205-206 °C
Thermal Conductivity
2.6 - 3.3 W/m.K
Electrical Properties
Dielectric Strength
15.4 kV/mm
Volume Resistivity
1 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm EP-3500 resin and its mixed systems with CoolTherm EP-3500 or EP-2000 Hardener before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Dark gray paste — CoolTherm EP-3500 resin as supplied
Viscosity 9,200 cP Resin at 60 °C; shear rate 10/sec
Specific gravity 2.98 — Resin at 25 °C
Mix ratio by weight 100:100 / 100:72 Resin:hardener EP-3500 Hardener / EP-2000 Hardener
Mix ratio by volume 100:100 / 100:78 Resin:hardener EP-3500 Hardener / EP-2000 Hardener
Mixed viscosity 8,000 / 3,800 cP At 60 °C; EP-3500 Hardener / EP-2000 Hardener
Mixed specific gravity 2.98 / 2.88 — EP-3500 Hardener / EP-2000 Hardener
Working life >3 / >3 hours At 60 °C; EP-3500 Hardener / EP-2000 Hardener
Shelf life 9 months Resin stored at 25 °C in the original, unopened container; periodic container rotation is required to reduce hard-packed filler settling
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm EP-3500 resin with EP-3500 or EP-2000 Hardener. Values are listed in that order and were measured after curing for 2 hours each at 120 °C, 150 °C, 180 °C, and 210 °C. Values are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 3.3 / 2.6 W/m·K EP-3500 Hardener / EP-2000 Hardener; test method not stated
Coefficient of linear thermal expansion 10.4 / 12 ppm/°C EP-3500 Hardener / EP-2000 Hardener; test method and temperature region not stated
Glass transition temperature 206 / 205 °C TMA; EP-3500 Hardener / EP-2000 Hardener
Hardness 90 / 93 Shore D ASTM D2240; EP-3500 Hardener / EP-2000 Hardener
Storage modulus 20 / — GPa DMA; EP-3500 Hardener / EP-2000 Hardener; EP-2000 Hardener value not reported
Volume resistivity 1 × 1014 / 1 × 1014 ohm-cm ASTM D257 at 25 °C; EP-3500 Hardener / EP-2000 Hardener
Dielectric strength 15.4 (390) / — kV/mm (V/mil) ASTM D149; EP-3500 Hardener / EP-2000 Hardener; EP-2000 Hardener value not reported