COOLTHERM DC-812

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM DC-812

Main features

  • Automotive Encapsulation Application
  • 1.4 x 10^16 ohm-cm Volume Resistivity
  • Resistance to Thermal Shock and Electrical Stability

Product Description

Thermoset DC-812 Epoxy Encapsulant is a two-component epoxy system developed specifically for potting high-voltage automotive ignition coils. The gray resin and amber hardener are processed at a 100:46 resin-to-hardener ratio by volume using automatic meter/mix/dispense equipment. The system combines low processing viscosity at elevated temperature with a cured Shore D hardness of 90, a volume resistivity of 1.4 × 1016 ohm-cm at 25 °C, and documented resistance to thermal shock. Its cured electrical properties support encapsulation applications requiring electrical stability at elevated temperatures.

Key features

  • Ignition-coil encapsulation: Developed specifically for potting high-voltage automotive ignition coils.
  • High electrical resistivity: Provides a typical cured volume resistivity of 1.4 × 1016 ohm-cm at 25 °C using ASTM D257.
  • Thermal-shock resistance: The cured epoxy system provides documented resistance to thermal shock and electrical stability at elevated temperature.

Applications / Suitable for

  • Potting high-voltage automotive ignition coils
  • Vacuum encapsulation using automatic meter/mix/dispense equipment
Product Family

COOLTHERM DC-812

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Resin: Gray Liquid | Hardener: Amber Liquid | Mixed: Tan Liquid
Specific Gravity
Resin: 1.55 | Hardener: 1.21 | Mixed: 1.46
Physical Properties
Viscosity (Part A)
(Resin) 60000 mPa.s
Viscosity (Part B)
(Hardener) 100 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed encapsulant before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Gray liquid / amber liquid / tan liquid — Resin / hardener / mixed material
Mix ratio 100:46 By volume DC-812 resin : DC-812 hardener
Viscosity — resin 60,000 cP At 25 °C; test method not stated
Viscosity — hardener 100 cP At 25 °C; test method not stated
Specific gravity 1.55 / 1.21 / 1.46 — Resin / hardener / mixed material at 25 °C
Gel time 20 minutes Mixed material at 121 °C
Working life 1–2 days Mixed material at 25 °C
Shelf life 6 months / 1 year — Resin / hardener from date of manufacture; stored at 25 °C in original, unopened containers
Technical properties

After-processing / final-state properties

Typical cured properties after a cure schedule of 2 hours at 90 °C followed by 2 hours at 120 °C. Values are not intended for specification purposes.

Property Value Unit Method / condition
Volume resistivity 1.4 × 1016 ohm-cm ASTM D257 at 25 °C
Coefficient of linear thermal expansion 32 ppm/°C ASTM D696
Hardness 90 Shore D ASTM D2240
Tensile strength 76.5 MPa ASTM D638
Elongation at break 3.2 % ASTM D638
Moisture absorption 0.26 % ASTM D570
Dielectric strength 500 V/mil ASTM D149
Dielectric constant 3.09 — ASTM D150 at 25 °C and 1 MHz